MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

EMS-Grivory Grivory® HT2VZ-15H PA6T/66-GF15
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 20% Glass Fiber Reinforced

Material Notes:

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³Dry; ISO 1183
Water Absorption 5.5 %5.5 %Sim. to ISO 62
Moisture Absorption 2.00 %2.00 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  82
@Time 15.0 sec
82
@Time 0.00417 hour
Conditioned; ISO 868
 84
@Time 15.0 sec
84
@Time 0.00417 hour
Dry; ISO 868
Tensile Strength at Break 100 MPa14500 psiConditioned; ISO 527-1/-2
 125 MPa18100 psiDry; ISO 527-1/-2
Elongation at Break 3.0 %3.0 %Dry; ISO 527-1/-2
 3.5 %3.5 %Conditioned; ISO 527-1/-2
Tensile Modulus 6.00 GPa870 ksiDry; ISO 527-1/-2
 6.00 GPa870 ksiConditioned; ISO 527-1/-2
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmDry; IEC 60093
 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 32.0 kV/mm813 kV/inConditioned; IEC 60243-1
 33.0 kV/mm838 kV/inDry; IEC 60243-1
Comparative Tracking Index 575 V575 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C16.7 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C41.7 µin/in-°FISO 11359-1/-2
Melting Point 310 °C590 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 140 °C284 °FLong Term; ISO 2578
 260 °C500 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 265 °C509 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 100 °C212 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Compressed air systems
 Fuel systems
 Hydraulic systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Energy distribution
 Mobile phones and other portable devices
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Tools & Accessories
ProcessingInjection Molding
Product AttributesCo Polyamide
 Improved alcohol resistance
 Partially aromatic Polyamide
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grivory® HT2V-15H PA6T/66-GF15
Celanese Zenite® 5145L BK010 LCP
DuPont Mobility and Materials Zytel® HTN 54G35EF NC010 Polyphthalamide (PPA)
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
Shandong Rike Chemical HELI™ HPA-221 PVC Processing Aid Series (PA)

PGRH389 / 157098

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.