Bostik 2106 Low viscosity, quick grab EVA Glue Stick
Categories:
Polymer
;
Adhesive
;
Thermoplastic
;
Ethylene Vinyl Acetate
;
Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Material Notes:
Bostik 2106 Low viscosity, quick grab EVA Glue Stick
Low viscosity. Quick grab for woodworking, general assembly and various plastics.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Viscosity
3700
cP
@Temperature 177 °C
3700
cP
@Temperature 350 °F
Typical
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
68.9
°C
156
°F
Minimum Service Temperature, Air
-17.8
°C
0.000
°F
Processing Properties
Metric
English
Comments
Pot Life
0.17
-
0.50
min
0.17
-
0.50
min
Open Time
Descriptive Properties
Color
Tan
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Bostik 2103 Flexible Bond EVA Glue Stick
Bostik 2107 General Purpose EVA Glue Stick
Bostik 2105 Low viscosity, short open time EVA Glue Stick
Bostik 2109 Economical, low viscosity EVA Glue Stick
Bostik 2102 Fast Setting EVA Glue Stick
PBOST09 / 27568
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.