MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

TIMCAL C-THERM™ 001 Graphite Additive for Thermally Conductive Polymers
Categories: Carbon; Carbon Black; Other Engineering Material; Additive/Filler for Polymer

Material Notes: The C-THERM line of high aspect ratio expanded graphite is designed to be added to polymers for the purpose of increasing the thermal conductivity of the resulting compound. Graphite's phonon collision mechanism of thermal conductivity plus its particle morphology allows high thermal conductivity of the compound at low levels of graphite loading, thus minimizing any abrasion problems.

Information provided by TIMCAL

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.150 g/cc0.00542 lb/in³Scott
Ash <= 0.3 %<= 0.3 %
 
Descriptive Properties
AspectFormSoft Granules

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group EP MAP-7.5 EPI Engineered Polymers Aliphatic Prepolymer
Graphite, Carbon, C
Avient Edgetek® PC-25GB-5GF/000 FR V-0 BLACK Polycarbonate (PC), Glass Filled
Indium Corp. Sn995 Cobalt-Doped, Pb-Free Soldering Alloy
NeoGraf eGRAF® SPREADERSHIELD™ SS1500 Graphite

CTIMCAL900 / 133499

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.