Description: A black thermoplastic high-flow elastomer for excellent injection molding performance with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and high quality SEBS compounds. It is polyolefin-based and UV stable. Supplied as free-flowing pellets in 20 kilogram (44 pound) moisture barrier bags. Features: - Water used as physical foaming agent
- Density range 0.95 to 0.15 depending on foaming agent
- Excellent ozone resistance