MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chemours Tefzel™ ETFE HT-2184 Premium fluoropolymer resin powder
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: Tefzel™ ETFE HT-2184 is a premium fluoropolymer resin in powder form. It provides the superior properties typical of fluoropolymer resins, such as excellent retention of properties after service, chemical inertness, and mechanical toughness. Applications: Tefzel™ ETFE HT-2184 is ideal for many end products, including chemical service items, such as lined valves and fittings, pump housings and impellers, column packings, and other abrasion resistant linings; high temperature electrical components and insulation; fasteners, corrugated tubing, and duct work; and film.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/ccASTM D792
Bulk Density 1.30 g/cc0.0470 lb/in³Chemours Test
Water Absorption 0.0070 %
@Time 86400 sec
0.0070 %
@Time 24.0 hour
ASTM D270
Melt Flow 6.0 g/10 min6.0 g/10 minASTM D3159
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7272ASTM D2240
Tensile Strength 40.0 MPa5800 psiASTM D638
Elongation at Break 250 %250 %ASTM D1457
Elongation, Ultimate 300 %300 %ASTM D638
Flexural Modulus 1.172 GPa170.0 ksiASTM D790
Flex Crack Resistance 10000 - 2700010000 - 27000Cycles MIT Folding Endurance; ASTM D2176
Izod Impact, Notched NBNBASTM D256
Coefficient of Friction 0.030 - 0.400.030 - 0.40ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
Dielectric Constant 2.5 - 2.62.5 - 2.6ASTM D1531
Dielectric Strength 70.0 kV/mm
@Thickness 0.250 mm
1780 kV/in
@Thickness 0.00984 in
ASTM D150
Dissipation Factor 0.0072
@Frequency 1e+6 Hz
0.0072
@Frequency 1e+6 Hz
ASTM D1531
Arc Resistance 122 sec122 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 - 280 °C491 - 536 °FNominal; ASTM D3418
Maximum Service Temperature, Air 155 °C311 °FUL 746
Flammability, UL94 V-0V-0
Oxygen Index 30 - 36 %30 - 36 %ASTM D2863
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Heat of Combustion13.7 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)1000ASTM B117. 5% NaCl at 35 °C (95 °F).
Weather and Chemical ResistanceExcellent
Weather Resistance (years unaffected)15Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8783 / 268709

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.