MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Vyncolit 4421 XB Novolac Phenolic
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral Filled

Material Notes: Mineral and organic filled phenolic molding compound with good mechanical properties.

USES: Fuse holders, brush holders, circuit breakers, automotive ignition and solenoid covers.

Information provided by Vyncolit, a Sumitomo Bakelite Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.650 g/cc0.0235 lb/in³Powder Density; ISO 60
Density 1.55 g/cc0.0560 lb/in³Relative Density; ISO 1183
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inInjection Molding; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psiISO 527
Elongation at Break 0.60 %0.60 %Tensile; ISO 527
Tensile Modulus 13.0 GPa1890 ksiISO 527
Flexural Strength 130 MPa18900 psiAt Rupture; ISO 178
Flexural Modulus 10.0 GPa1450 ksiISO 178
Flexural Strain at Break 1.4 %1.4 %ISO 178
Compressive Strength 240 MPa34800 psiISO 604
Charpy Impact Unnotched 0.800 J/cm²3.81 ft-lb/in²ISO 179
Charpy Impact, Notched 0.250 J/cm²1.19 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 1.00e+9 - 1.00e+10 ohm1.00e+9 - 1.00e+10 ohmDry; IEC 167
Dielectric Strength 25.0 kV/mm635 kV/inIEC 243
Comparative Tracking Index 175 V175 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature 20.0 °C
22.2 µin/in-°F
@Temperature 68.0 °F
TMA
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 20.0 °C
27.8 µin/in-°F
@Temperature 68.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75 Af
Flammability, UL94  V-1
@Thickness 1.60 mm
V-1
@Thickness 0.0630 in
 V-0
@Thickness 4.00 mm
V-0
@Thickness 0.157 in
Shrinkage 0.15 %0.15 %Post Shrinkage; ISO 2577
 
Descriptive Properties
ColorBlack
ISO typePF 2 C3
Main FillerMineral & Organic
Molding MethodCompression, transfer, injection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Raschig Group DECAL® 937 Phenolic
Raschig Group DECAL® 152CL Phenolic
Plenco 5118 Phenolic, Granular, Compression Molded
Plenco 4300 Phenolic, Granular, Compression Molded
Overview of materials for Phenolic; Unreinforced; Molded

PVYNC038 / 72246

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.