MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBAFLEX P D40.3 HR FC TPC-ET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Polyester elastomer, Shore D39, suitable for food contact applications

Properties: flexible, good gliding properties, good recovery behavior, High wear resistance, compliant for food contact (according to 10/2011 EC), semi-crystalline

Typical areas of application: Sealing elements, Seals, Bellows, Spring elements, Sliding elements, Haptic components, industrial goods, Piston, Rollers, Hoses, Valves, Timing belt

Industries: Automotive, Electrical and electronics industry, Household appliances, Industry, Agriculture, Food processing industry, Mechanical Engineering, Medical Technology, Furniture industry, Sanitary industry, Sports & Recreation

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183-1
Linear Mold Shrinkage, Flow 0.0110 cm/cm0.0110 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0100 cm/cm0.0100 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 39.039.0DIN ISO 7619-1
Tensile Strength at Break 21.0 MPa3050 psiISO 527-1
Elongation at Break 800 %800 %ISO 527-1
Charpy Impact Unnotched 10.0 J/cm²47.6 ft-lb/in²ISO 179-1eU
 
Thermal PropertiesMetricEnglishComments
Melting Point 195 °C383 °FISO 11357-1/-3
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 240 °C374 - 464 °F
Mold Temperature 30.0 - 80.0 °C86.0 - 176 °F
Drying Temperature 100 °C212 °F
Dry Time 3.00 - 6.00 hour3.00 - 6.00 hour
Moisture Content <= 0.0400 %<= 0.0400 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO510 / 326584

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.