MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Teijin Films Melinex® 1311 Polyester Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® 1311 is a clear polyester film with antistatic properties on both surfaces for improved web handling and safety.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 96.5 MPa14000 psiASTM D882A
Film Tensile Strength at Yield, TD 100 MPa14500 psiASTM D882A
Film Elongation at Break, MD 160 %160 %ASTM D882A
Film Elongation at Break, TD 120 %120 %ASTM D882A
Coefficient of Friction, Dynamic 0.600.60A-B; ASTM D1894
Film Tensile Strength at Break, MD 193 MPa28000 psiASTM D882A
Film Tensile Strength at Break, TD 241 MPa35000 psiASTM D882A
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 2.00e+10 ohm
@Temperature 25.0 °C
2.00e+10 ohm
@Temperature 77.0 °F
500 V DC @ 54% RH; ASTM D257
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 4.0 %
@Temperature 190 °C,
Time 300 sec
4.0 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %
@Temperature 190 °C,
Time 300 sec
1.0 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  88.2 %
@Thickness 0.127 mm
88.2 %
@Thickness 0.00500 in
TLT; ASTM D1003
 88.4 %
@Thickness 0.102 mm
88.4 %
@Thickness 0.00400 in
TLT; ASTM D1003
 88.5 %
@Thickness 0.0762 mm
88.5 %
@Thickness 0.00300 in
TLT; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 051 Polyester Film, 380 Gauge
DuPont Teijin Films Melinex® 054 Polyester Film
DuPont Teijin Films Melinex® 238 Polyester Film
DuPont Teijin Films Melinex® 454 Polyester Film, 92 Gauge
DuPont Teijin Films Melinex® 197 Polyester Film

PDTZ9009 / 139420

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.