System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Radici Radilon® A 42K 100 M NT Polyamide 66
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Extruded
;
Nylon 66, Heat Stabilized
Material Notes:
PA66 high viscosity extrusion grade. Heat stabilized. Natural color. Suitable for extrusion of tubes, profiles, bars, rods and sheets. Also suitable for injection molding of high thickness items.
Information provided by Radici Group.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.14
g/cc
0.0412
lb/in³
DAM; ISO 1183
Water Absorption
8.4 %
@Thickness 2.00 mm,
Temperature 23.0 °C
8.4 %
@Thickness 0.0787 in,
Temperature 73.4 °F
Immersion; ISO 62
Moisture Absorption
2.10 %
@Thickness 2.00 mm,
Temperature 23.0 °C
2.10 %
@Thickness 0.0787 in,
Temperature 73.4 °F
50% RH; ISO 62
Viscosity Test
260
cm³/g
2.60
dl/g
Viscosity Index; Sulfuric Acid; ISO 307
Linear Mold Shrinkage, Flow
0.011
cm/cm
0.011
in/in
DAM; ISO 294-4
0.013
cm/cm
0.013
in/in
Conditioned; ISO 294-4
Linear Mold Shrinkage, Transverse
0.013
cm/cm
0.013
in/in
ISO 294-4
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
60.0
MPa
8700
psi
50mm/min. Conditioned; ISO 527-2/1A
85.0
MPa
12300
psi
50mm/min. DAM; ISO 527-2/1A
Elongation at Break
45 %
45 %
50mm / min. DAM; ISO 527-2/1A
>= 50 %
>= 50 %
50 mm / min. Conditioned; ISO 527-2/1A
Elongation at Yield
4.5 %
4.5 %
DAM; ISO 527-2/1A
25 %
25 %
Conditioned; ISO 527-2/1A
Tensile Modulus
1.60
GPa
232
ksi
1mm / min. Conditioned; ISO 527-2/1A
3.20
GPa
464
ksi
1mm / min. DAM; ISO 527-2/1A
Flexural Strength
110
MPa
16000
psi
2mm / min. DAM; ISO 178
Flexural Modulus
2.90
GPa
421
ksi
2mm / min. DAM; ISO 178
Charpy Impact, Notched
0.500
J/cm²
@Temperature -30.0 °C
2.38
ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
0.600
J/cm²
@Temperature -30.0 °C
2.86
ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
2.00
J/cm²
@Temperature -30.0 °C
9.52
ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1e/A
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+11
ohm-cm
1.00e+11
ohm-cm
Conditioned. 500V; IEC 60093
1.00e+13
ohm-cm
1.00e+13
ohm-cm
DAM; 500V.; IEC 60093
Surface Resistance
1.00e+10
ohm
1.00e+10
ohm
Conditioned; IEC 60093
1.00e+12
ohm
1.00e+12
ohm
DAM; 500V.; IEC 60093
Thermal Properties
Metric
English
Comments
Melting Point
260
°C
500
°F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi)
195
°C
383
°F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi)
75.0
°C
167
°F
ISO 75/2Af
Vicat Softening Point
240
°C
@Load 5.10 kg
464
°F
@Load 11.2 lb
50°C/h; ISO 306
Flammability, UL94
HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Flame Spread
0.000
mm/min
@Thickness 3.00 mm
0.000
in/min
@Thickness 0.118 in
Automotive Interior; ISO 3795
Glow Wire Flammability Index
750
°C
@Thickness 2.00 mm
1380
°F
@Thickness 0.0787 in
IEC 60695-2-1/2
Processing Properties
Metric
English
Comments
Processing Temperature
270
-
290
°C
518
-
554
°F
Extrusion Temperature
Melt Temperature
280
-
300
°C
536
-
572
°F
Injection Molding
Mold Temperature
70.0
-
90.0
°C
158
-
194
°F
Descriptive Properties
Injection Molding Injection Speed
Medium
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PRADI6911 / 293416
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.