MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

AISI E9310 Steel, normalized at 890°C (1635°F)
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 9000 Series Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel

Key Words: SAE J770, UNS G93106, AMS 6260F, AMS 6265B, ASTM A322, ASTM A519, ASTM A711, SAE J404
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 269269
Hardness, Knoop 294294Converted from Brinell
Hardness, Rockwell B 9999Converted from Brinell
Hardness, Rockwell C 2727Converted from Brinell hardness value.
Hardness, Vickers 284284Converted from Brinell hardness value.
Tensile Strength, Ultimate 910 MPa132000 psi
Tensile Strength, Yield 570 MPa82700 psi
Elongation at Break 18.8 %18.8 %in 50 mm
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel.
Poissons Ratio 0.290.29Calculated
Machinability 50 %50 %hot rolled and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPa11600 ksiTypical for steels.
Izod Impact 119 J87.8 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000174 ohm-cm0.0000174 ohm-cmEstimated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.5 µm/m-°C
@Temperature 20.0 °C
6.39 µin/in-°F
@Temperature 68.0 °F
Estimated
 12.2 µm/m-°C
@Temperature 250 °C
6.78 µin/in-°F
@Temperature 482 °F
Estimated
 13.9 µm/m-°C
@Temperature 500 °C
7.72 µin/in-°F
@Temperature 932 °F
Estimated
 14.7 µm/m-°C
@Temperature 1000 °C
8.17 µin/in-°F
@Temperature 1830 °F
Estimated
Specific Heat Capacity 0.472 J/g-°C0.113 BTU/lb-°FEstimated
Thermal Conductivity 51.9 W/m-K360 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.080 - 0.13 %0.080 - 0.13 %
Chromium, Cr 1.0 - 1.4 %1.0 - 1.4 %
Iron, Fe 93.77 - 95.19 %93.77 - 95.19 %As remainder
Manganese, Mn 0.45 - 0.65 %0.45 - 0.65 %
Molybdenum, Mo 0.080 - 0.15 %0.080 - 0.15 %
Nickel, Ni 3.0 - 3.5 %3.0 - 3.5 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si 0.20 - 0.35 %0.20 - 0.35 %
Sulfur, S <= 0.025 %<= 0.025 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI E9310 Steel, normalized at 890°C (1635°F), 100 mm (4 in.) round
AISI E9310 Steel, annealed at 845°C (1550°F)
AISI E9310 Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, 830°C (1525°F) reheat, 150°C (300°F) temper
AISI E9310 Steel, direct quenched from pot, tempered at 230°C (450°F), 0.99 mm case depth
AISI E9310 Steel, double quenched and tempered at 150°C (300°F), 1.4 mm case depth

M931AT / 8668

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.