MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled; Polycarbonate (PC)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.962 - 1.48 g/cc0.0348 - 0.0535 lb/in³Average value: 1.27 g/cc Grade Count:165
 1.02 - 1.07 g/cc
@Temperature 260 - 260 °C
0.0368 - 0.0387 lb/in³
@Temperature 500 - 500 °F
Average value: 1.05 g/cc Grade Count:2
Filler Content 5.00 - 40.0 %5.00 - 40.0 %Average value: 17.2 % Grade Count:42
Water Absorption 0.100 - 0.600 %0.100 - 0.600 %Average value: 0.327 % Grade Count:40
Moisture Absorption at Equilibrium 0.0200 - 0.320 %0.0200 - 0.320 %Average value: 0.179 % Grade Count:33
Water Absorption at Saturation 0.250 - 0.700 %0.250 - 0.700 %Average value: 0.517 % Grade Count:10
Additive Loading 10.0 - 30.0 %10.0 - 30.0 %Average value: 16.7 % Grade Count:6
Viscosity  8.00 - 8.00 cP
@Temperature 260 - 260 °C
8.00 - 8.00 cP
@Temperature 500 - 500 °F
Average value: 121000 cP Grade Count:1
 8.00 - 8.00 cP
@Load 5.00 - 5.00 kg
8.00 - 8.00 cP
@Load 11.0 - 11.0 lb
Average value: 121000 cP Grade Count:1
 115000 - 185000 cP
@Frequency 1000 - 1000 Hz
115000 - 185000 cP
@Frequency 1000 - 1000 Hz
Average value: 121000 cP Grade Count:3
 115000 - 185000 cP
@Temperature 260 - 260 °C
115000 - 185000 cP
@Temperature 500 - 500 °F
Average value: 121000 cP Grade Count:3
Maximum Moisture Content 0.0200 - 0.04000.0200 - 0.0400Average value: 0.0222 Grade Count:9
Linear Mold Shrinkage 0.00100 - 0.00700 cm/cm0.00100 - 0.00700 in/inAverage value: 0.00325 cm/cm Grade Count:122
 0.00400 - 0.00550 cm/cm
@Temperature 80.0 - 80.0 °C
0.00400 - 0.00550 in/in
@Temperature 176 - 176 °F
Average value: 0.00475 cm/cm Grade Count:2
Linear Mold Shrinkage, Transverse 0.00100 - 0.00800 cm/cm0.00100 - 0.00800 in/inAverage value: 0.00422 cm/cm Grade Count:35
 0.00550 - 0.00600 cm/cm
@Temperature 80.0 - 80.0 °C
0.00550 - 0.00600 in/in
@Temperature 176 - 176 °F
Average value: 0.00575 cm/cm Grade Count:2
Melt Flow 1.00 - 41.0 g/10 min1.00 - 41.0 g/10 minAverage value: 14.5 g/10 min Grade Count:92
Ash 9.50 - 22.0 %9.50 - 22.0 %Average value: 14.1 % Grade Count:11
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 82.0 - 12182.0 - 121Average value: 114 Grade Count:30
Tensile Strength, Ultimate 27.0 - 131 MPa3920 - 19000 psiAverage value: 81.5 MPa Grade Count:121
 5.00 - 50.0 MPa
@Temperature 60.0 - 120 °C
725 - 7250 psi
@Temperature 140 - 248 °F
Average value: 26.0 MPa Grade Count:1
Tensile Strength, Yield 48.8 - 124 MPa7080 - 18000 psiAverage value: 78.2 MPa Grade Count:52
Elongation at Break 0.600 - 109 %0.600 - 109 %Average value: 4.98 % Grade Count:128
 3.00 - 70.0 %
@Temperature 60.0 - 120 °C
3.00 - 70.0 %
@Temperature 140 - 248 °F
Average value: 26.3 % Grade Count:1
Elongation at Yield 2.00 - 10.0 %2.00 - 10.0 %Average value: 3.99 % Grade Count:16
 2.00 - 2.00 %
@Temperature 60.0 - 120 °C
2.00 - 2.00 %
@Temperature 140 - 248 °F
Average value: 2.00 % Grade Count:1
Modulus of Elasticity 2.41 - 13.0 GPa350 - 1890 ksiAverage value: 5.43 GPa Grade Count:78
 1.30 - 3.60 GPa
@Temperature 60.0 - 120 °C
189 - 522 ksi
@Temperature 140 - 248 °F
Average value: 2.73 GPa Grade Count:1
Flexural Yield Strength 57.0 - 186 MPa8270 - 27000 psiAverage value: 121 MPa Grade Count:121
Flexural Modulus 2.20 - 10.3 GPa319 - 1500 ksiAverage value: 5.08 GPa Grade Count:132
Izod Impact 112 - 150 J82.6 - 111 ft-lbAverage value: 128 J Grade Count:5
Izod Impact, Notched 0.278 - 4.27 J/cm0.520 - 8.00 ft-lb/inAverage value: 0.967 J/cm Grade Count:98
 0.300 - 1.60 J/cm
@Temperature -50.0 - 0.000 °C
0.562 - 3.00 ft-lb/in
@Temperature -58.0 - 32.0 °F
Average value: 0.741 J/cm Grade Count:7
 0.588399 - 0.686465 J/cm
@Temperature -30.0 - -30.0 °C
1.10231 - 1.28603 ft-lb/in
@Temperature -22.0 - -22.0 °F
Average value: 0.741 J/cm Grade Count:2
 0.588399 - 0.686465 J/cm
@Thickness 3.17 - 6.35 mm
1.10231 - 1.28603 ft-lb/in
@Thickness 0.125 - 0.250 in
Average value: 0.741 J/cm Grade Count:2
Izod Impact, Unnotched 0.747 - 8.01 J/cm1.40 - 15.0 ft-lb/inAverage value: 5.18 J/cm Grade Count:28
Izod Impact, Notched (ISO) 5.00 - 23.0 kJ/m²2.38 - 10.9 ft-lb/in²Average value: 9.89 kJ/m² Grade Count:18
 10.0 - 10.0 kJ/m²
@Temperature -30.0 - -30.0 °C
4.76 - 4.76 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 10.0 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 30.0 - 37.0 kJ/m²14.3 - 17.6 ft-lb/in²Average value: 33.7 kJ/m² Grade Count:6
 40.0 - 40.0 kJ/m²
@Temperature -30.0 - -30.0 °C
19.0 - 19.0 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 40.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.50 - 9.00 J/cm²11.9 - 42.8 ft-lb/in²Average value: 4.64 J/cm² Grade Count:26
 3.40 - 3.80 J/cm²
@Temperature -30.0 - -20.0 °C
16.2 - 18.1 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 3.57 J/cm² Grade Count:6
Charpy Impact, Notched 0.300 - 3.20 J/cm²1.43 - 15.2 ft-lb/in²Average value: 1.05 J/cm² Grade Count:45
 0.300 - 1.20 J/cm²
@Temperature -30.0 - -20.0 °C
1.43 - 5.71 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 0.681 J/cm² Grade Count:13
Dart Drop, Total Energy 18.0 - 34.0 J13.3 - 25.1 ft-lbAverage value: 23.7 J Grade Count:3
Instrumented Impact Total Energy 5.65 - 17.0 J4.17 - 12.5 ft-lbAverage value: 11.6 J Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 10000 - 1.00e+16 ohm-cm10000 - 1.00e+16 ohm-cmAverage value: 3.04e+15 ohm-cm Grade Count:38
Surface Resistance 1e+05 - 1.00e+16 ohm1e+05 - 1.00e+16 ohmAverage value: 1.91e+15 ohm Grade Count:29
Static Decay 0.500 - 2.00 sec0.500 - 2.00 secAverage value: 1.75 sec Grade Count:6
Dielectric Constant 2.80 - 3.302.80 - 3.30Average value: 3.11 Grade Count:11
Dielectric Strength 27.0 - 35.0 kV/mm686 - 889 kV/inAverage value: 31.3 kV/mm Grade Count:12
Dissipation Factor 0.00200 - 0.01000.00200 - 0.0100Average value: 0.00564 Grade Count:11
Comparative Tracking Index 100 - 350 V100 - 350 VAverage value: 199 V Grade Count:14
 
Thermal PropertiesMetricEnglishComments
CTE, linear 26.0 - 61.2 µm/m-°C14.4 - 34.0 µin/in-°FAverage value: 41.7 µm/m-°C Grade Count:28
 3.10 - 3.90 µm/m-°C
@Temperature 40.0 - 100 °C
1.72 - 2.17 µin/in-°F
@Temperature 104 - 212 °F
Average value: 3.50 µm/m-°C Grade Count:2
CTE, linear, Transverse to Flow 52.0 - 82.0 µm/m-°C28.9 - 45.6 µin/in-°FAverage value: 71.8 µm/m-°C Grade Count:11
 6.40 - 6.50 µm/m-°C
@Temperature 40.0 - 100 °C
3.56 - 3.61 µin/in-°F
@Temperature 104 - 212 °F
Average value: 6.45 µm/m-°C Grade Count:2
Specific Heat Capacity 1.56 - 2.15 J/g-°C0.373 - 0.514 BTU/lb-°FAverage value: 1.82 J/g-°C Grade Count:5
Thermal Conductivity 0.142 - 0.260 W/m-K0.985 - 1.80 BTU-in/hr-ft²-°FAverage value: 0.189 W/m-K Grade Count:5
Maximum Service Temperature, Air 80.0 - 115 °C176 - 239 °FAverage value: 100 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 92.0 - 146 °C198 - 295 °FAverage value: 126 °C Grade Count:58
Deflection Temperature at 1.8 MPa (264 psi) 51.0 - 160 °C124 - 320 °FAverage value: 120 °C Grade Count:141
Vicat Softening Point 95.0 - 160 °C203 - 320 °FAverage value: 125 °C Grade Count:64
 130 - 130 °C
@Temperature 50.0 - 50.0 °C
266 - 266 °F
@Temperature 122 - 122 °F
Average value: 130 °C Grade Count:3
 130 - 130 °C
@Load 5.10 - 5.10 kg
266 - 266 °F
@Load 11.2 - 11.2 lb
Average value: 130 °C Grade Count:3
UL RTI, Electrical 60.0 - 80.0 °C140 - 176 °FAverage value: 62.2 °C Grade Count:8
UL RTI, Mechanical with Impact 60.0 - 80.0 °C140 - 176 °FAverage value: 62.2 °C Grade Count:8
UL RTI, Mechanical without Impact 60.0 - 80.0 °C140 - 176 °FAverage value: 62.2 °C Grade Count:8
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:112
Oxygen Index 24.0 - 33.0 %24.0 - 33.0 %Average value: 25.5 % Grade Count:6
Glow Wire Test 650 - 960 °C1200 - 1760 °FAverage value: 829 °C Grade Count:7
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 300 °C356 - 572 °FAverage value: 247 °C Grade Count:19
Nozzle Temperature 220 - 310 °C428 - 590 °FAverage value: 267 °C Grade Count:25
Melt Temperature 210 - 310 °C410 - 590 °FAverage value: 259 °C Grade Count:99
Mold Temperature 40.0 - 130 °C104 - 266 °FAverage value: 76.6 °C Grade Count:116
Injection Velocity 40.0 - 540 mm/sec1.57 - 21.3 in/secAverage value: 240 mm/sec Grade Count:5
Drying Temperature 26.7 - 121 °C80.0 - 250 °FAverage value: 91.6 °C Grade Count:103
Moisture Content 0.0100 - 0.0500 %0.0100 - 0.0500 %Average value: 0.0229 % Grade Count:42
Dew Point -40.0 - -28.9 °C-40.0 - -20.0 °FAverage value: -29.7 °C Grade Count:14
Injection Pressure 60.0 - 150 MPa8700 - 21800 psiAverage value: 96.9 MPa Grade Count:31
Vent Depth 0.00381 cm0.00150 inAverage value: 0.00381 cm Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled
Overview of materials for Polycarbonate, Molded
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive
Overview of materials for PC/ABS + Stainless Steel

O1171a / 89061

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.