MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC
Categories: Ceramic; Glass; Glass Ceramic; Machinable Ceramic; Oxide

Material Notes: Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and coefficient of thermal expansion similar to most metals and sealing glasses. Machines to tight tolerances up to 0.0005”, surface finish of less than 20µin, and polishes to a smoothness of 0.5µin. Used for ultra high vacuum, aerospace, nuclear, wielding, fixturing, and medical applications. Readily machined and no firing required. Bars, disks, rods and plates are available fro 1/16” thick up to 12” diameter.

Vendors: Aremco offers a range of machinable ceramics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.52 g/cc0.0910 lb/in³
Water Absorption 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 4848
Flexural Strength 94.0 MPa13600 psi
Compressive Strength 345 MPa50000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmDC
Dielectric Constant 6.0
@Frequency 1e+6 Hz
6.0
@Frequency 1e+6 Hz
Dielectric Strength 30.9 kV/mm785 kV/in
Dielectric Loss Index 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.6 µm/m-°C7.00 µin/in-°F
Thermal Conductivity 1.50 W/m-K10.4 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 800.0 °C1472 °FOxidizing
Maximum Service Temperature, Inert 800 °C1470 °F
 800 °C1470 °FVacuum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Accuratus MACOR Machinable Glass Ceramic
Corning Macor® Machinable Glass Ceramic
Astro Met Macor® Machinable Glass Ceramic
Morgan Advanced Ceramics MACOR® Mac-MGCW Machinable glass ceramic
Advanced Ceramics ACL 2089 Cordierite

CAREM12 / 553

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.