MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SK Chemicals Saran® 525 PVDC  (discontinued **)
Categories: Polymer; Thermoplastic; Polyvinyl Dichloride (PVDC); Polyvinyl Dichloride (PVDC)

Material Notes: SARAN® 525 barrier polymer, a copolymer of vinylidene chloride and vinyl chloride, designed for sheet coextrusion and forming into rigid plastic barrier containers for food applications. It is supplied as a white free flowing powder (particle size 240-320 microns). It offers excellent oxygen barrier, unaffected by humidity and complies with the requirements of FDA for use as a component of articles in contact with food.

SK Global Chemical has purchased the SARAN® resin business from Dow.

Key Words: Polyvinyl Dichloride
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.73 g/cc0.0625 lb/in³
Oxygen Transmission 0.00400 cc-mm/m²-24hr-atm0.0102 cc-mil/100 in²-24hr-atm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SK Chemicals Saran® 469 PVDC
SK Chemicals Saran® F-239 PVDC
SK Chemicals Saran® 516 PVDC
SK Chemicals Saran® 867 PVDC
SK Chemicals Saran® MA 119 PVDC

PDW539 / 34608

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.