MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Goodfellow Multi Wall Carbon Nanotube Powder (MWCNT)
Categories: Carbon

Material Notes: Multi Wall Carbon Nanotube (MWCNT) powder is produced via Catalytic Chemical Vapor Deposition (CCVD). The carbon nanotubes are tube-shaped materials, exclusively composed of carbon atoms, having a nanometric diameter. The graphite layer can be visualized somewhat like a rolled-up wire with a continuous unbroken hexagonal mesh and carbon atoms at the apexes of the hexagons. With action of van der Waals forces, carbon nanotubes tend to cluster into bundles or agglomerates. Consequently, carbon nanotubes look like a black powder. At nanoscale, they have a spaghetti-like structure.

Primary interest is in applications requiring low electrical percolation threshold such as high-performance electrostatic dissipative plastics or coatings. These carbon nanotubes are used in various applications in different markets:

  • Transportation (Automotive, Aeronautic, Boats)
  • Electronics (Electronic packaging, EMI-shielding, sensors)
  • Energy (Lithium-ion)
  • Industrial applications (Oil&Gas, dynamic rubber parts, coatings, heating elements)
  • Sporting goods
Benefits:
  • High electrical conductivity
  • Good processability
  • Retention of key mechanical properties
  • Cost effective
  • High recyclability in thermoplastics
  • Cleanliness
  • Flame retardancy (synergy in combination with other flame retardants)
  • Thermal dissipation
  • UV resistance
  • Black tinting

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Surface Area 250 - 300 m²/g250 - 300 m²/gBET
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.00010 ohm-cm0.00010 ohm-cm
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 90 %90 %Carbon Purity; TGA
 
Descriptive Properties
Average Diameter9.5 nmTEM
Average Length1.5 µmTEM
Purity - Amorphous Carbonnone detectedHigh resolution Transmission Electron Microscopy (HRTEM)
Purity - Transition Metal Oxide<1%ICP-MS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CGOODF090e / 239186

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.