MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Baldcypress Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Softwood. Relatively easy to work with hand tools. Data is based on small, clear, air-dried samples unless specified.

Key Words: Taxodium distichum; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.460 g/cc0.0166 lb/in³Air Dry (12-15% Moisture Content)
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.0730 GPa10.6 ksiIn Bending
Flexural Yield Strength 49.6 MPa7190 psiBending stress at proportional limit
Flexural Modulus 9.70 - 9.94 GPa1410 - 1440 ksiIn Bending
Compressive Strength 6.20 MPa899 psiPerpendicular to Grain
 44.0 - 44.1 MPa6380 - 6400 psiParallel to Grain
Poissons Ratio 0.3260.326µLT, 12% Moisture Content
 0.3380.338µLR, 12% Moisture Content
 0.3560.356µTR, 12% Moisture Content
 0.4110.411µRT, 12% Moisture Content
Shear Strength 6.90 MPa1000 psiOrientation Unknown
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.110 W/m-K0.760 BTU-in/hr-ft²-°FOven Dry
 0.133 W/m-K0.920 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 3.8 %3.8 %Radial; Green to Zero Moisture
 6.2 %6.2 %Tangential; Green to Zero Moisture
 10.5 %10.5 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alerce Wood
American Balsam Fir Wood
Morgan Advanced Ceramics Kao-Lok® Hardware for Blanket Wallpaper Systems 310 SS Washers and Studs
Abarco (Albarco) Wood
African Mahogany Wood

PTSAC / 71286

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.