System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Sumitomo Bakelite North America Epiall® 1960B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Categories:
Polymer
;
Thermoset
;
Epoxy
;
Epoxy, Encapsulating, Glass or Mineral Filled
;
Filled/Reinforced Thermoset
Material Notes:
Epiall 1960B-1 is a mineral and short fiberglass filled epoxy compound, formulated for the encapsulation of passive electronic devices.
Information provided by Sumitomo Bakelite North America, Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.76
g/cc
0.0636
lb/in³
ASTM D792
Water Absorption
0.20 %
@Temperature 50.0 °C,
Time 173000 sec
0.20 %
@Temperature 122 °F,
Time 48.0 hour
ASTM D570
Linear Mold Shrinkage
0.0030
-
0.0050
cm/cm
0.0030
-
0.0050
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
80.0
MPa
11600
psi
ASTM D638
Flexural Strength
115
MPa
16700
psi
at rupture; ASTM D790
Flexural Modulus
12.4
GPa
1800
ksi
ASTM D790
Compressive Strength
242
MPa
35100
psi
ASTM D695
Izod Impact, Notched
0.370
J/cm
0.693
ft-lb/in
ASTM D256
Electrical Properties
Metric
English
Comments
Dielectric Constant
4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
wet; ASTM D150
Dielectric Strength
12.9
kV/mm
@Frequency 60 Hz
328
kV/in
@Frequency 60 Hz
step-by-step, wet; ASTM D149
14.9
kV/mm
@Frequency 60 Hz
378
kV/in
@Frequency 60 Hz
short time, wet; ASTM D149
Dissipation Factor
0.019
@Frequency 1e+6 Hz
0.019
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance
180
sec
180
sec
ASTM D495
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
275
°C
527
°F
Post Baked; ASTM D648A
Descriptive Properties
Color
Black
Form
Granular
Molding Method
Compression
Transfer
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Sumitomo Bakelite EPIALL 1960B-1 Epoxy Molding Compound
G-10 Fiberglass Epoxy Laminate Sheet
Sumitomo Bakelite North America E 3812M-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Sumitomo Bakelite North America Epiall® 1904B-1 Short Glass Fiber Reinforced Epoxy
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
P90X904 / 142679
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.