MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® B BK X146 EM1 LT K1 PA6-I
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Vydyne B BK X146 EM1 LT K1 is a general-purpose, impact-modified PA6 resin. Available in black, it is inorganic heat-stabilized for improved resistance to high temperatures. It is lubricated for machine feed and easy mold release and shows an improved impact resistance also at low temperatures.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³DAM; ISO 1183
Moisture Absorption at Equilibrium 2.6 %2.6 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.014 cm/cm
@Thickness 2.00 mm
0.014 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.018 cm/cm
@Thickness 2.00 mm
0.018 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5080 psi50% RH; ISO 527-2
 60.0 MPa8700 psiDAM; ISO 527-2
Elongation at Break 45 %45 %DAM; ISO 527-2
 55 %55 %50% RH; ISO 527-2
Elongation at Yield 5.5 %5.5 %DAM; ISO 527-2
 7.0 %7.0 %50% RH; ISO 527-2
Tensile Modulus 1.20 GPa174 ksi50% RH; ISO 527-2
 2.00 GPa290 ksiDAM; ISO 527-2
Izod Impact, Notched (ISO)  9.00 kJ/m²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 12.0 kJ/m²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 450 V
@Thickness 3.00 mm
450 V
@Thickness 0.118 in
IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 150 °C302 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FUnannealed; DAM; ISO 75-2/A
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 270 °C446 - 518 °FInjection
Middle Barrel Temperature 230 - 270 °C446 - 518 °FInjection
Front Barrel Temperature 230 - 270 °C446 - 518 °FInjection
Nozzle Temperature 230 - 270 °C446 - 518 °FInjection
Melt Temperature 230 - 270 °C446 - 518 °FInjection
Mold Temperature 80.0 - 90.0 °C176 - 194 °FInjection
Drying Temperature 80.0 - 90.0 °C176 - 194 °FInjection
Dry Time >= 3.00 hour>= 3.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
AppearanceBlack
FeaturesAbrasion Resistance
 Chemical Resistant
 Gasoline Resistant
 Good Impact Strength
 Good Mold Release
 Good Toughness
 Heat Aging Resistant
 High Elongation
 Impact Modified
 Low Temperature Impact Resistance
 Lubricated
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9285 / 287638

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.