MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Akulon® F136 PA6, Very High Viscosity, Film Extrusion
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Film Grade

Material Notes: Very High Viscosity, Film Extrusion

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Water Vapor Transmission 35.0 g/m²/day2.25 g/100 in²/dayDIS 15106-1/-3
Oxygen Transmission 1.35 cc-mm/m²-24hr-atm3.43 cc-mil/100 in²-24hr-atm0% RH; DIS 15105-1/-2
 1.95 cc-mm/m²-24hr-atm4.95 cc-mil/100 in²-24hr-atm85% RH; DIS 15105-1/-2
Viscosity 2250 cP
@Temperature 260 °C
2250 cP
@Temperature 500 °F
Melt; DSM Method
 50 cP
@Shear Rate 10000 1/s,
Temperature 280 °C
50 cP
@Shear Rate 10000 1/s,
Temperature 536 °F
 50 cP
@Shear Rate 10000 1/s,
Temperature 260 °C
50 cP
@Shear Rate 10000 1/s,
Temperature 500 °F
 50 cP
@Shear Rate 10000 1/s,
Temperature 240 °C
50 cP
@Shear Rate 10000 1/s,
Temperature 464 °F
 900 cP
@Shear Rate 100 1/s,
Temperature 280 °C
900 cP
@Shear Rate 100 1/s,
Temperature 536 °F
 1000 cP
@Shear Rate 100 1/s,
Temperature 260 °C
1000 cP
@Shear Rate 100 1/s,
Temperature 500 °F
 1030 cP
@Shear Rate 100 1/s,
Temperature 240 °C
1030 cP
@Shear Rate 100 1/s,
Temperature 464 °F
 1030 cP
@Shear Rate 0.1 1/s,
Temperature 280 °C
1030 cP
@Shear Rate 0.1 1/s,
Temperature 536 °F
 1200 cP
@Shear Rate 0.1 1/s,
Temperature 260 °C
1200 cP
@Shear Rate 0.1 1/s,
Temperature 500 °F
 1300 cP
@Shear Rate 0.1 1/s,
Temperature 240 °C
1300 cP
@Shear Rate 0.1 1/s,
Temperature 464 °F
Viscosity Number 245 cm³/g2.45 dl/gISO 307, 1157, 1628
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 34.0 MPa4930 psiISO 527-3
Film Elongation at Break, MD 350 %350 %ISO 527-3
Modulus of Elasticity 0.450 GPa65.3 ksi50 mm/min; DSM Method
Coefficient of Friction, Dynamic 1.01.0ISO 8295
Tear Strength Test 3232Trouser Tear resistance, parallel; ISO 6383-1
Film Tensile Strength at Break, MD 83.0 MPa12000 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-1/-2
Specific Heat Capacity 1.55 J/g-°C0.370 BTU/lb-°F
 2.25 J/g-°C
@Temperature 20.0 - 150 °C
0.538 BTU/lb-°F
@Temperature 68.0 - 302 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 83 %83 %DSM Method
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 °C518 °FExtruder
Die Temperature 270 °C518 °F
Roll Temperature 110 °C230 °FChill
 
Descriptive Properties
Puncture resistance1400 J/mDSM Method
RSV formic acid3.6[1g/100ml], DSM Method
Type of extrusionCast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allvac® REX 734™ UNS S31675 Specialty Steel
Akro-Plastic Akromid® B3 1 black (2501) PA 6 Dry, Heat Stabilized
BASF Ultramid® B27 03 PA6
BASF Ultramid® B40 L PA6
BASF Ultramid® B40 LN PA6

PDSM8011 / 184712

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.