MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

INEOS Styrolution Lustran® SAN 31 Styrene Acrylonitrile (SAN)
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Transparent

Material Notes: Lustran® SAN 31 is a transparent styrene acrylonitrile (SAN) with high flow and toughness. Good chemical and heat resistance, Meets USP Class VI requirements, Meets FDA modified ISO 10993-1 requirements, UL classification 94 HB. Applications: Dinnerware, Medical devices, Cosmetic packaging, Tumblers, mugs and jars, Lens

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ASTM D 792
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm0.0030 - 0.0040 in/inASTM D 955
Melt Flow 7.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8383ASTM D 785
Tensile Strength 72.4 MPa10500 psiASTM D 638
Tensile Modulus 3.28 GPa476 ksiASTM D 638
Flexural Strength 115 MPa16700 psiASTM D 790
Flexural Modulus 3.45 GPa500 ksiASTM D 790
Izod Impact, Notched 0.214 J/cm
@Temperature 23.0 °C
0.400 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 2.03 J/cm
@Temperature 23.0 °C
3.80 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 68.4 µm/m-°C38.0 µin/in-°FASTM D 696
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C205 °Funannealed; ASTM D 648
 103 °C217 °Fannealed; ASTM D 648
Vicat Softening Point 110 °C
@Load 1.02 kg
230 °F
@Load 2.25 lb
B/2 120C/H; ASTM D 1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.571.57Sodium D Line; ASTM D 542
Haze 0.70 %0.70 %ASTM D 1003
Transmission, Visible 87 - 88 %
@Wavelength 550 nm
87 - 88 %
@Wavelength 550 nm
ASTM D 1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 218 - 260 °C424 - 500 °F
Mold Temperature 38.0 - 82.0 °C100 - 180 °F
Drying Temperature 82.0 - 88.0 °C180 - 190 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Styrolux® 656C SBC
Ineos Nova Zylar® 221 Clear Impact Modified Acrylic Copolymer
A. Schulman Diamond SAN 267 Styrene Acrylonitrile, Transparent Engineering Thermoplastic
INEOS Styrolution Lustran® SAN Sparkle Styrene Acrylonitrile (SAN)
Denka TX-100S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene

PSTYR9833 / 216060

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.