MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trelleborg Emerson & Cuming Stycast® 4640-25 Two-Component Silicone Flexible Encapsulant
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Emerson & Cuming 4640-25 Stycast® Two-Component Silicone Flexible Encapsulant
Description

An RTV condensation cure. Pourable and room temperature curable.

Features
  • High Temperature
  • Poor Chemical Resistance
  • Filled
  • Mix Ratio (by weight) = 100:0.4
Cure Type: Room Temp or Heat Bonding Type: Silicone

The Stycast® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.750 g/cc0.0271 lb/in³
Viscosity 45000 cP
@Temperature 25.0 °C
45000 cP
@Temperature 77.0 °F
Mixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.0
@Frequency 1e+6 Hz
2.0
@Frequency 1e+6 Hz
Dielectric Strength 9.84 kV/mm250 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 240 - 360 min4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow SE 9184 WHITE RTV
Dow SE 738 SILICONE RTV
Dow SE 4486 SILICONE RTV
Dow SE 4422 SILICONE RTV
Dow 3-4680 SILICONE GEL KIT

PEMERS04 / 35696

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.