MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Redwood Plastics Redco™ CPVC
Categories: Polymer; Thermoplastic; Vinyl (PVC); Chlorinated PVC (CPVC)

Material Notes:

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 - 1.57 g/cc0.0553 - 0.0567 lb/in³ASTM D792
Water Absorption  0.030 %
@Thickness 3.17 mm,
Time 86400 sec
0.030 %
@Thickness 0.125 in,
Time 24.0 hour
73°F; ASTM D570
 0.55 %
@Thickness 3.17 mm,
Time 86400 sec
0.55 %
@Thickness 0.125 in,
Time 24.0 hour
212°F; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 119119ASTM D785
Tensile Strength 55.2 MPa8010 psiASTM D638
Tensile Modulus >= 2.4821 GPa>= 360.00 ksiASTM D638
Flexural Strength 104 MPa15100 psiASTM D790
Flexural Modulus 2.8613 GPa415.00 ksiASTM D790
Compressive Strength 69.6 MPa10100 psiASTM D695
Compressive Modulus 1.35 GPa196 ksiASTM D695
Izod Impact, Notched 0.801 J/cm1.50 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.34e+15 ohm-cm1.34e+15 ohm-cm50% RH; ASTM D257
Dielectric Constant 3.7
@Frequency 3000 - 3800 Hz
3.7
@Frequency 3000 - 3800 Hz
ASTM D150
Dielectric Strength 49.2 kV/mm
@Thickness 3.17 mm
1250 kV/in
@Thickness 0.125 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 61.2 µm/m-°C34.0 µin/in-°FASTM D696
Thermal Conductivity 0.137 W/m-K0.951 BTU-in/hr-ft²-°FASTM C177
Heat Distortion Temperature 102.8 °C217.0 °FASTM D648
Flammability, UL94 V-0V-0
 5VB5VB
 5VA5VA
Oxygen Index 60 %60 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW121 / 296687

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.