MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66, 10% Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Carbon Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.10 - 1.70 g/cc0.0397 - 0.0614 lb/in³Average value: 1.23 g/cc Grade Count:46
Filler Content 5.00 - 50.0 %5.00 - 50.0 %Average value: 15.0 % Grade Count:7
Water Absorption 0.450 - 2.50 %0.450 - 2.50 %Average value: 1.09 % Grade Count:18
Moisture Absorption at Equilibrium 1.90 - 2.70 %1.90 - 2.70 %Average value: 2.18 % Grade Count:14
Water Absorption at Saturation 1.80 - 8.00 %1.80 - 8.00 %Average value: 5.74 % Grade Count:13
Linear Mold Shrinkage 0.00100 - 0.0180 cm/cm0.00100 - 0.0180 in/inAverage value: 0.00550 cm/cm Grade Count:30
 0.00200 - 0.00300 cm/cm
@Temperature 80.0 - 80.0 °C
0.00200 - 0.00300 in/in
@Temperature 176 - 176 °F
Average value: 0.00250 cm/cm Grade Count:4
Linear Mold Shrinkage, Transverse 0.000 - 0.0110 cm/cm0.000 - 0.0110 in/inAverage value: 0.00792 cm/cm Grade Count:13
 0.00700 - 0.00800 cm/cm
@Temperature 80.0 - 80.0 °C
0.00700 - 0.00800 in/in
@Temperature 176 - 176 °F
Average value: 0.00750 cm/cm Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110 - 125110 - 125Average value: 114 Grade Count:8
Tensile Strength, Ultimate 82.7 - 650 MPa12000 - 94300 psiAverage value: 153 MPa Grade Count:38
Tensile Strength, Yield 105 - 200 MPa15200 - 29000 psiAverage value: 148 MPa Grade Count:8
Elongation at Break 1.00 - 8.00 %1.00 - 8.00 %Average value: 3.62 % Grade Count:42
Modulus of Elasticity 4.69 - 55.0 GPa680 - 7980 ksiAverage value: 10.2 GPa Grade Count:37
Flexural Yield Strength 117 - 630 MPa17000 - 91400 psiAverage value: 227 MPa Grade Count:28
Flexural Modulus 3.59 - 42.0 GPa520 - 6090 ksiAverage value: 9.59 GPa Grade Count:29
Flexural Strain at Break 2.80 - 4.20 %2.80 - 4.20 %Average value: 3.33 % Grade Count:3
Izod Impact, Notched 0.370 - 2.03 J/cm0.693 - 3.80 ft-lb/inAverage value: 0.946 J/cm Grade Count:17
 0.5339 - 0.5339 J/cm
@Temperature -40.0 - -40.0 °C
1.000 - 1.000 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 0.534 J/cm Grade Count:1
 0.5339 - 0.5339 J/cm
@Thickness 3.17 - 3.17 mm
1.000 - 1.000 ft-lb/in
@Thickness 0.125 - 0.125 in
Average value: 0.534 J/cm Grade Count:1
Izod Impact, Unnotched 4.27 - 10.1 J/cm8.00 - 19.0 ft-lb/inAverage value: 6.89 J/cm Grade Count:10
Izod Impact, Notched (ISO) 5.00 - 15.0 kJ/m²2.38 - 7.14 ft-lb/in²Average value: 9.13 kJ/m² Grade Count:7
 4.00 - 5.00 kJ/m²
@Temperature -30.0 - -30.0 °C
1.90 - 2.38 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 4.67 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 28.0 - 28.0 kJ/m²
@Temperature -30.0 - -30.0 °C
13.3 - 13.3 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 28.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 1.50 - 7.50 J/cm²7.14 - 35.7 ft-lb/in²Average value: 4.28 J/cm² Grade Count:24
 2.20 - 6.00 J/cm²
@Temperature -40.0 - -30.0 °C
10.5 - 28.6 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 3.46 J/cm² Grade Count:9
Charpy Impact, Notched 0.300 - 4.50 J/cm²1.43 - 21.4 ft-lb/in²Average value: 0.859 J/cm² Grade Count:23
 0.300 - 0.500 J/cm²
@Temperature -40.0 - -30.0 °C
1.43 - 2.38 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 0.429 J/cm² Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.500 - 1.00e+13 ohm-cm0.500 - 1.00e+13 ohm-cmAverage value: 2.94e+11 ohm-cm Grade Count:21
Surface Resistance 1.00 - 1.00e+13 ohm1.00 - 1.00e+13 ohmAverage value: 2.51e+11 ohm Grade Count:23
Insulation Resistance 1000 - 100000 ohm1000 - 100000 ohmAverage value: 67000 ohm Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.00 - 79.2 µm/m-°C1.67 - 44.0 µin/in-°FAverage value: 38.5 µm/m-°C Grade Count:13
Melting Point 221 - 265 °C430 - 509 °FAverage value: 258 °C Grade Count:22
Maximum Service Temperature, Air 90.0 - 220 °C194 - 428 °FAverage value: 148 °C Grade Count:11
Deflection Temperature at 0.46 MPa (66 psi) 210 - 260 °C410 - 500 °FAverage value: 246 °C Grade Count:18
Deflection Temperature at 1.8 MPa (264 psi) 177 - 259 °C350 - 498 °FAverage value: 237 °C Grade Count:32
Vicat Softening Point 200 - 253 °C392 - 487 °FAverage value: 241 °C Grade Count:8
Glass Transition Temp, Tg 5.00 - 72.0 °C41.0 - 162 °FAverage value: 40.2 °C Grade Count:3
Flammability, UL94 HB - V-0HB - V-0Grade Count:19
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 310 °C518 - 590 °FAverage value: 286 °C Grade Count:5
Nozzle Temperature 270 - 300 °C518 - 572 °FAverage value: 283 °C Grade Count:5
Melt Temperature 250 - 310 °C482 - 590 °FAverage value: 287 °C Grade Count:26
Mold Temperature 65.6 - 121 °C150 - 250 °FAverage value: 91.2 °C Grade Count:27
Drying Temperature 75.0 - 120 °C167 - 248 °FAverage value: 85.8 °C Grade Count:23
Moisture Content 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.152 % Grade Count:9
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:3
Injection Pressure 68.9 - 124 MPa10000 - 18000 psiAverage value: 103 MPa Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 63, 35% Glass-Filled
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
Overview of materials for Nylon 66, 10% Glass Fiber Filled
Overview of materials for Nylon 6, 10% Glass Fiber Filled
Overview of materials for Nylon 66, 40% Carbon Fiber Filled

O2521 / 78020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.