MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chemours Teflon™ PFA 450HP Special purpose fluoroplastic resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: Teflon™ PFA 450HP is a special purpose fluoroplastic resin available in pellet form. This resin is a chemically modified form of Teflon™ PFA 350 that combines many of the benefits of the parent resin (highest resistance to environmental stress-cracking with a typical MIT folding endurance of 500,000*) with several additional benefits including enhanced purity, improved thermal stability while processing, and chemical inertness; for example, to ozonated fluids. Applications for Teflon™ PFA 450HP include tubing, chemical linings for pipes, valves, and fittings used in the chemical processing industries, unsupported pipe linings for the production of ultra-pure chemicals, semiconductor components, and fluid handling components for high performance chemical delivery systems where purity in the parts-per billion range is needed. Teflon™ PFA 450HP is preferred in applications where extended service is required in hostile environments involving chemical, thermal, and mechanical stress.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.15 g/cc2.15 g/ccASTM D792
Water Absorption <= 0.030 %
@Time 86400 sec
<= 0.030 %
@Time 24.0 hour
ASTM D570
Melt Flow 2.0 g/10 min2.0 g/10 minASTM D3307
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength  14.0 MPa
@Temperature 250 °C
2030 psi
@Temperature 482 °F
ASTM D3307
 28.0 MPa
@Temperature 23.0 °C
4060 psi
@Temperature 73.4 °F
ASTM D3307
Elongation, Ultimate  300 %
@Temperature 23.0 °C
300 %
@Temperature 73.4 °F
ASTM D3307
 500 %
@Temperature 250 °C
500 %
@Temperature 482 °F
ASTM D3307
Flexural Modulus  0.0690 GPa
@Temperature 250 °C
10.0 ksi
@Temperature 482 °F
ASTM D790
 0.625 GPa
@Temperature 23.0 °C
90.6 ksi
@Temperature 73.4 °F
ASTM D790
Flex Crack Resistance 500000
@Thickness 0.203 mm
500000
@Thickness 0.00800 in
Cycles MIT Folding Endurance; ASTM D2176
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm>= 1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+17 ohm>= 1.00e+17 ohmASTM D257
Dielectric Constant 2.03
@Frequency 1e+6 Hz
2.03
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 80.0 kV/mm
@Thickness 0.250 mm
2030 kV/in
@Thickness 0.00984 in
Short Time; ASTM D149
Dissipation Factor 0.00020
@Frequency 1e+6 Hz
0.00020
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 180 sec>= 180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Melting Point 305 °C581 °FASTM D4591
Maximum Service Temperature, Air 260 °C500 °FContinuous, per accelerated heat-aging test
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Critical Shear Rate (1/s)12372°C
Heat of Combustion5.3 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)1000ASTM B117. 5% NaCl at 35 °C (95 °F).
Weather and Chemical ResistanceOutstanding
Weather Resistance (years unaffected)10Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8806 / 268732

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.