MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Hifax TKC 519X C1 BLACK High Impact Polypropylene, Mineral Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced, Impact Modified

Material Notes: HIFAX TKC 519X C1 Black is a mineral reinforced, impact modified polypropylene copolymer for injection molding. It combines very high rigidity with a low coefficient of linear thermal expansion (CLTE) and very good processability for body panel applications. The grade has been specifically designed for molding of large complex parts that require good dimensional.

Availability: Asia-Pacific

Application: Body Panels; Exterior Automotive Applications

Market: Automotive

Processing Method: Injection Molding

Attribute: Good Dimensional Stability; Good Impact Resistance; Good Processability; Impact Modified; Low Shrinkage; Paintable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183-1/A
Melt Flow 16.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
16.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 20.0 MPa2900 psiISO 527-1, -2
Flexural Modulus 2.80 GPa406 ksiISO 178
Izod Impact, Notched (ISO)  3.50 kJ/m²
@Temperature -30.0 °C
1.67 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 25.0 kJ/m²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9130 / 324065

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.