Description: AKROMID B3 GF 30 RM-M natural (3291) is a 30% glass fiber reinforced polyamide 6 with high stiffness and strength, limited moisture absorption and light inherent color. Applications are housings and other dimensional stable parts in the automotive and electronic industry. Features: - High Stiffness
- High Strength
- Good Dimensional Stability
- Low to No Water Absorption
Uses:- Automotive Application
- Electrical/Electronic Applications
- Housings
Information provided by Akro-Plastic GmbH |