MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Titanium Transage 129, Triplex Heat Treat 760/650/480°C
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: This alloy has very good fatigue resistance, which is enhanced by an alpha-beta anneal at 650ºC before aging at 425-540ºC.

Characteristics:

  • Martensitic alloy
  • High hardenability
  • Heat treatable
  • Good fatigue properties
  • Good fracture properties
  • Suitable for hot-working and cold-forming

See other heat treatments for this alloy as well as entries for Transage 134 and 175.

Key Words: Ti-11.5V-2Al-2Sn-11Zr; T129
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.82 g/cc0.174 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1190 MPa173000 psi
Tensile Strength, Yield 1100 MPa160000 psi
Elongation at Break 8.0 %8.0 %
Modulus of Elasticity 108 GPa15700 ksiAfter Duplex Heat Treat 815/540ºC
Poissons Ratio 0.330.33Typical for beta titanium alloy.
Shear Modulus 40.6 GPa5890 ksiCalculated from typical values.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000150 ohm-cm0.000150 ohm-cmEstimated from similar high-V-stabilized beta titanium alloys.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.50 µm/m-°C
@Temperature 20.0 - 100 °C
4.72 µin/in-°F
@Temperature 68.0 - 212 °F
Typical beta titanium alloy
 9.20 µm/m-°C
@Temperature 0.000 - 315 °C
5.11 µin/in-°F
@Temperature 32.0 - 599 °F
Typical Mo-stabilized-beta titanium alloy
Specific Heat Capacity 0.525 J/g-°C0.125 BTU/lb-°FTypical value for titanium alloys.
Thermal Conductivity 7.80 W/m-K54.1 BTU-in/hr-ft²-°FEstimated from similar high-V-stabilized beta titanium alloys.
Beta Transus 720 °C1330 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.0 %2.0 %
Boron, B <= 0.030 %<= 0.030 %
Carbon, C <= 0.080 %<= 0.080 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.20 %<= 0.20 %
Nitrogen, N <= 0.050 %<= 0.050 %
Other, each <= 0.10 %<= 0.10 %
Other, total <= 0.40 %<= 0.40 %
Oxygen, O <= 0.15 %<= 0.15 %
Tin, Sn 2.0 %2.0 %
Titanium, Ti 73.5 %73.5 %
Vanadium, V 11.5 %11.5 %
Yttrium, Y <= 0.0050 %<= 0.0050 %
Zirconium, Zr 11 %11 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) Solution Treated
Titanium Ti-13V-11Cr-3Al; (Ti-13-11-3) Annealed 850°C (1560°F) + Aged 510°C 8 hr
Titanium Ti-13V-2.7Al-7Sn-2Zr, ST 815°C, Aged 540°C (1000°F)
Ti15Mo5Zr3Al ß titanium alloy
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Alpha-Beta Forged, RA

MTB291 / 14174

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.