MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman tetra-DUR F 4308 Bulk Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: UL-licensed

Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stability, color retention, chemical stability, zero shrink/class-A-surface, and uniform color.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 - 1.80 g/cc0.0578 - 0.0650 lb/in³ISO 1138
Linear Mold Shrinkage 0.00 - 0.0020 cm/cm0.00 - 0.0020 in/inprocessing; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 40.0 - 50.0 MPa5800 - 7250 psiISO 527
Flexural Strength 100 - 140 MPa14500 - 20300 psiISO 178
Flexural Modulus 8.00 - 12.0 GPa1160 - 1740 ksiISO 178
Compressive Strength 140 - 160 MPa20300 - 23200 psiISO 604
Charpy Impact Unnotched 2.00 - 4.50 J/cm²9.52 - 21.4 ft-lb/in²ISO 179
Charpy Impact, Notched 2.00 - 4.50 J/cm²9.52 - 21.4 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 4.5
@Frequency 100 Hz
4.5
@Frequency 100 Hz
IEC 60250
Dielectric Strength 29.0 kV/mm
@Thickness 1.00 mm
737 kV/in
@Thickness 0.0394 in
IEC 60243
Dielectric Loss Index <= 0.030
@Frequency 100 Hz
<= 0.030
@Frequency 100 Hz
IEC 60250
Arc Resistance 190 sec190 secASTM D495-61
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 - 30.0 µm/m-°C11.1 - 16.7 µin/in-°FVDE 0304T1
Deflection Temperature at 1.8 MPa (264 psi) >= 240 °C>= 464 °FISO 75
Flammability, UL94 V-0V-0
Shrinkage 0.00 - 0.050 %0.00 - 0.050 %post molding; ISO 2577
 
Descriptive Properties
Water Absorption>40 mg/1dISO 62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman tetra-DUR F 4401 Bulk Molding Compound
A. Schulman tetra-DUR F 4209 Bulk Molding Compound
A. Schulman tetra-DUR F 4206 Bulk Molding Compound
A. Schulman tetra-DUR L 4305 Bulk Molding Compound
A. Schulman tetra-DUR F 4001 Bulk Molding Compound

PBMC911 / 123375

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.