System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Epsan Epimix PBT GFR 10 NC Q1B001 Polybutylene Terephthalate
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
Material Notes:
EPIMIX PBT, reinforced with 10% of glass fiber, heat stabilized, superior gloss, lubricated for injection molding. EPIMIX PBT GFR 10 is used in all sectors of industry, compliance with RoHs derivatives.
Information provided by Epsan Plastik
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.34
g/cc
0.0484
lb/in³
ISO 1183
Linear Mold Shrinkage
0.0040
cm/cm
0.0040
in/in
Parallel; ISO 294-4
0.010
cm/cm
0.010
in/in
Normal; ISO 294-4
Ash
10 %
10 %
ISO 3451-4
Mechanical Properties
Metric
English
Comments
Tensile Stress
80.0
MPa
11600
psi
ISO 527-2
Elongation at Break
2.0 %
2.0 %
ISO 527-2
Tensile Modulus
4.50
GPa
653
ksi
ISO 527-2
Flexural Strength
110
MPa
16000
psi
ISO 178
Flexural Modulus
4.30
GPa
624
ksi
ISO 178
Izod Impact, Notched (ISO)
6.00
kJ/m²
2.86
ft-lb/in²
ISO 180/1A
Charpy Impact, Notched
0.800
J/cm²
3.81
ft-lb/in²
ISO 179/1eA
Thermal Properties
Metric
English
Comments
Melting Point
220
°C
428
°F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi)
208
°C
406
°F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi)
195
°C
383
°F
ISO 75-2/A
Vicat Softening Point
210
°C
410
°F
ISO 306/B50
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
EN 60695-11-10
Processing Properties
Metric
English
Comments
Processing Temperature
260
°C
500
°F
Recommended Injection Molding Temperature
Drying Temperature
80.0
°C
176
°F
Average Drying Time is 2-4 hrs
Moisture Content
0.20 %
0.20 %
ISO 15512
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Epsan Epimix PBT NC Q101 Polybutylene Terephthalate
Epsan Epimix PBT IMP NC Q1B801 Polybutylene Terephthalate
Epsan Epimix PBT GFR 30 NC Q1D001 Polybutylene Terephthalate
Epsan Epimix PBT GV0 30 NC Q1D0B301 Polybutylene Terephthalate
Epsan Epimix PBT FV0 NC Q1B301 Polybutylene Terephthalate, Halogenated
PEPSAN072 / 186386
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.