MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Akro-Plastic Akromid® A3 K1 FR PA Fire Resistant  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: With completion of the AKROMID® FR series (Flame Retardant), AKRO-PLASTIC is able to deal with its Polyamide 6 and 6.6 with nearly all requirements in the area of electro- and electronic applications. According to the company‘s philosophy of AKRO-PLASTIC, self-evidently all products of the AKROMID® FR series are free of halogens, do not contain one of the prohibited bromine types and can be colored into almost every color due to the non-available red phosphorus. All materials correspond to the RoHS Directive 2002/95/EG for limitation of use of hazardous substances in electro- and electronic devices and are authorized according to the REACh Regulation EG 1907/2006. Due to the fact, that AKROMID® FR types are free of halogens, the adherence to the regulation WEEE 2002/96/EG is simplified by the OEM. That is the fact, because a separate collection of the raw-material must not be considered here. A comparison to Polyamide, not containing flame-protection definitely shows comparable dates with regard to modulus of rigidity as well as tensile stress at break. With regard to those features, AKROMID® FR outmatches types of polyamide in similar application areas including brominated- and what is more anorganic flame protection systems not requiring an extremely high filling level. Furthermore, data representing toughness like elongation at break and impact strength substantiate the significant predominance. A further requirement of globally acting users is the avoidance of deposit of emissions on conducting contacts among special climatical conditions. This undesired migrational effect is not available at any version due to the applied flame retardant. In this way, parts of AKROMID® FR are even applicable in subtropical areas.

Application:
Housing parts for ground fault circuit interrupters, sliding valves and automatic circuit breakers
Switchboard parts
Circuit breakers and circuit breaker elements
Plugs, plug applications and connection plug boards

Information from Akro-Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 500 - 600 V500 - 600 V
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 5VA5VA
Glow Wire Ignition Temperature 775 °C1430 °FIEC 60695-2-13

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond DIAMALOY 730 ABS/PC Alloy, Flame Retardant
A. Schulman Diamond ABSPC 7430-1005T ABS/PC Injection Molding Grade
Shinkong Synthetic Fibers Shinite® F602G30 Nylon 66, 30% Glass Filled, Fire Retardant, Halogen Free
DuPont Mobility and Materials Hytrel® HTR8136BK TPC-ET
Celanese Hytrel® 3046 NC010 TPC-ET

PAKRO096 / 126876

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.