MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or blow molding. It is polyolefin based and completely recyclable.

Key Features:

  • UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
  • Neutral, easy coloring formulation.
  • Used in sealing applications.
  • EU and China RoHS compliant.
Applications:
  • Industrial - Architectural and Construction
Uses:
  • Construction Applications
  • Glazing
  • Expansion Joint
  • Outdoor Applications
Processing Method: Blow Molding, Extrusion Blow Molding, Injection Blow Molding, Injection Molding and Multi Injection Molding

Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D792
Maximum Moisture Content 0.0800.080
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 64642 mm, 15 sec; ISO 868
Tensile Strength at Break 5.70 MPa827 psiAcross flow; ASTM D412
Tensile Stress at Strain 2.20 MPa
@Strain 100 %
319 psi
@Strain 100 %
Across flow; ASTM D412
Elongation at Break 470 %470 %Across flow; ASTM D412
Compression Set  32 %
@Temperature 70.0 °C,
Time 79200 sec
32 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
 60 %
@Temperature 125 °C,
Time 252000 sec
60 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395B
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.3
@Thickness 2.01 mm
2.3
@Thickness 0.0791 in
ASTM D150
Dielectric Strength 31.1 kV/mm
@Thickness 2.03 mm
790 kV/in
@Thickness 0.0799 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -62.8 °C-81.0 °FASTM D746
UL RTI, Electrical 100 °C212 °FUL 746
UL RTI, Mechanical with Impact 85.0 °C185 °FUL 746
Flammability, UL94  HB
@Thickness 1.10 mm
HB
@Thickness 0.0433 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
Rear Barrel Temperature 177 - 191 °C351 - 376 °F
Middle Barrel Temperature 179 - 193 °C354 - 379 °F
Front Barrel Temperature 185 - 199 °C365 - 390 °F
Nozzle Temperature 185 - 210 °C365 - 410 °F
Die Temperature 177 - 216 °C351 - 421 °FExtrusion
Melt Temperature 143 - 216 °C289 - 421 °FProcessing
 179 - 216 °C354 - 421 °FExtrusion
Mold Temperature 23.9 - 51.7 °C75.0 - 125 °F
Drying Temperature 82.0 °C180 °F
Dry Time 3 hour3 hour
Back Pressure 0.345 - 0.689 MPa50.0 - 99.9 psi
Clamp Pressure 41.0 - 69.0 MPa5950 - 10000 psi
Vent Depth 0.00254 cm0.00100 in
Cushion 0.317 - 0.635 cm0.125 - 0.250 in
Screw Speed 100 - 200 rpm100 - 200 rpm
 
Descriptive Properties
Injection RateFast
Max Regrind20%
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
A. Schulman Alcryn® 1060 BK Melt Processable Rubber
A. Schulman DuraGrip™ DGR 6160 NC Thermoplastic Elastomer (TPE)
A. Schulman DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE)
A. Schulman Alcryn® 2060 NC Melt Processable Rubber

PADW160 / 22878

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.