MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Tenite 572A1V95316 Cellulose Acetate Butyrate, Smoke, Trsp  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate Butyrate, Molded

Material Notes: Applications:
  • Molded parts

Product Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucents. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Cellulose Acetate Butyrate 572-16 contains an odor mask lubricant and an ultra-violet inhibitor (UVI). It has a plasticizer level of 16%.

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Water Absorption 1.2 %
@Time 86400 sec
1.2 %
@Time 24.0 hour
Immersion; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 6060ASTM D785
Tensile Strength at Break 31.0 MPa4500 psiASTM D638
Tensile Strength, Yield 30.3 MPa4390 psiASTM D638
Elongation at Break 26 %26 %ASTM D638
Flexural Modulus 1.162 GPa168.5 ksiASTM D790
Izod Impact, Notched  1.02 J/cm
@Temperature -40.0 °C
1.91 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 5.31 J/cm
@Temperature 23.0 °C
9.95 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C174 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C153 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Descriptive Properties
Formula Number572UVI; odor mask
Plasticizer16 percent
Weight Loss on Heating0.9 percentASTM D707, 72 hrs, 80°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tenite Propionate 358A4000018 Clear, Trsp Cellulose Acetate Propionate
Eastman Tenite Propionate 376E4000012 Clear, Trsp Cellulose Acetate Propionate
Eastman Tenite Acetate 105E2R30025 Natural, Trsp Cellulose Acetate
Eastman Tenite Propionate 380A2R30018 Natural, Trsp Cellulose Acetate Propionate
Eastman Tenite Propionate 381E4000015 Clear, Trsp Cellulose Acetate Propionate

PE8830 / 129675

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.