MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AdvanSix Capran® Oxyshield® OXTR (Retortable Grade, 1.0 mil) Monoaxially Oriented Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Film Grade

Material Notes: Description: Capran® Oxyshield™ Oriented Ultra Barrier Retortable Grade is a monoaxially oriented, co-extruded nylon 6-based clear film having excellent gas barrier through a broad range of relative humidity. The film provides high strength, good chemical resistance, and excellent flavor and aroma barrier for food packaging.

Former Honeywell product; AdvanSix is a spin-off of Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0420 lb/in³Yield Density
Water Vapor Transmission 181 g/m²/day
@Temperature 37.8 °C
11.7 g/100 in²/day
@Temperature 100 °F
97%RH; ASTM F1249
Oxygen Transmission Rate 1.04 cc/m²/day0.0670 cc/100 in²/day73°F (23°F) / 65%RH; ASTM D3985
 1.23 cc/m²/day0.0792 cc/100 in²/day73°F (23°C) / 0%RH; ASTM D3985
Thickness 25.4 microns1.00 mil
Surface Tension >= 56 dynes/cm>= 56 dynes/cmtreated side; ASTM D2578
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 87 %87 %ASTM D882
Film Elongation at Break, TD 413 %413 %ASTM D882
Coefficient of Friction 0.200.20film to stainless steel; ASTM D1894
 0.500.50film to film; ASTM D1894
Tear Strength Test 732732graves tear MD, grams/mil; ASTM D1004
 11921192graves tear TD, grams/mil; ASTM D1004
Film Tensile Strength at Break, MD 241 MPa35000 psiASTM D882
Film Tensile Strength at Break, TD 99.3 MPa14400 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air <= 93.0 °C<= 199 °Fcontinuous use temperature
 <= 176 °C<= 349 °Fshort time use temperature
Shrinkage, MD 11 %
@Treatment Temp. 177 °C,
Time 601 sec
11 %
@Treatment Temp. 350 °F,
Time 0.167 hour
ASTM D1204
Shrinkage, TD 1.6 %
@Treatment Temp. 177 °C,
Time 601 sec
1.6 %
@Treatment Temp. 350 °F,
Time 0.167 hour
ASTM D1204
 
Optical PropertiesMetricEnglishComments
Haze <= 5.5 %<= 5.5 %ASTM D1003
Transmission, Visible 90 %90 %clear; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexWeb® HRH-10 - 3/8 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb
DIAB Divilette® 650 HV Polyester Resin-based Core Bedding Adhesive

PALC031 / 23793

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.