MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hippe PVDF  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated polymers in terms of dielectricity.

Information provided by Hippe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.79 g/cc1.79 g/ccDIN 53 479
Moisture Absorption at Equilibrium <= 0.050 %<= 0.050 %Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation <= 0.050 %<= 0.050 %DIN 53 495
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 105 MPa
@Time 30.0 sec
15200 psi
@Time 0.00833 hour
DIN 53 456
Tensile Strength 55.0 MPa7980 psiDIN 53 455
Elongation at Break 20 - 400 %20 - 400 %DIN 53 455
Tensile Modulus 2.00 GPa290 ksiDIN 53 457
Flexural Modulus 2.00 GPa290 ksifrom bending test; DIN 53 457
Charpy Impact, Notched NBNBDIN 53 453
Coefficient of Friction, Dynamic 0.300.30Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+14 ohm-cm4.00e+14 ohm-cmDIN 53 482, VDE 0303, Part 3
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmDIN 53 482
Dielectric Constant 8.0
@Frequency 1e+6 Hz
8.0
@Frequency 1e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 17.0 - 150 kV/mm432 - 3810 kV/inBreakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.060
@Frequency 1e+6 Hz
0.060
@Frequency 1e+6 Hz
DIN 53 483, IEC-250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 130 µm/m-°C72.2 µin/in-°F
Specific Heat Capacity 1.20 J/g-°C0.287 BTU/lb-°F
Thermal Conductivity 0.110 W/m-K0.763 BTU-in/hr-ft²-°F
Melting Point 178 °C352 °FDIN 53 736
Maximum Service Temperature, Air 150 °C302 °FContinuous use
 150 °C302 °FShort Periods
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °FISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO-R 75 Method A
Glass Transition Temp, Tg -18.0 °C-0.400 °Fdynamic; DIN 53 736
Flammability, UL94 V-0V-0
 
Descriptive Properties
Colorwhite
Creep ResistanceGrade CTI 600DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, sudsresistant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride - extruded products
GEHR Plastics PVDF Polyvinylidene Fluoride
Adamas Lakinor® U PVDF
CENTROPLAST CENTROFLON Polyvinylidene fluoride
Evonik Dyflor® EE PVDF

PHIPPE996 / 122000

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.