MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Glass Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 - 1.45 g/cc0.0412 - 0.0524 lb/in³Average value: 1.25 g/cc Grade Count:40
Filler Content 10.0 - 30.0 %10.0 - 30.0 %Average value: 20.0 % Grade Count:3
Water Absorption 0.0600 - 0.150 %0.0600 - 0.150 %Average value: 0.0884 % Grade Count:25
Moisture Absorption at Equilibrium 0.00600 - 0.0600 %0.00600 - 0.0600 %Average value: 0.0240 % Grade Count:3
Water Absorption at Saturation 0.200 - 0.220 %0.200 - 0.220 %Average value: 0.205 % Grade Count:4
Linear Mold Shrinkage 0.00100 - 0.0690 cm/cm0.00100 - 0.0690 in/inAverage value: 0.00449 cm/cm Grade Count:38
Linear Mold Shrinkage, Transverse 0.00300 - 0.00500 cm/cm0.00300 - 0.00500 in/inAverage value: 0.00450 cm/cm Grade Count:4
Melt Flow 3.00 - 24.0 g/10 min3.00 - 24.0 g/10 minAverage value: 14.1 g/10 min Grade Count:20
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 60.0 - 148 MPa8700 - 21500 psiAverage value: 93.4 MPa Grade Count:23
Tensile Strength, Yield 50.0 - 140 MPa7250 - 20300 psiAverage value: 93.9 MPa Grade Count:15
Elongation at Break 1.00 - 20.0 %1.00 - 20.0 %Average value: 4.39 % Grade Count:39
Modulus of Elasticity 3.80 - 10.6 GPa551 - 1540 ksiAverage value: 6.71 GPa Grade Count:12
Flexural Yield Strength 80.0 - 216 MPa11600 - 31300 psiAverage value: 145 MPa Grade Count:40
Flexural Modulus 3.00 - 12.0 GPa435 - 1740 ksiAverage value: 6.18 GPa Grade Count:32
Izod Impact, Notched 0.641 - 1.30 J/cm1.20 - 2.44 ft-lb/inAverage value: 0.966 J/cm Grade Count:10
 0.694 - 0.694 J/cm
@Temperature -40.0 - -40.0 °C
1.30 - 1.30 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 0.694 J/cm Grade Count:1
Izod Impact, Unnotched 3.36 - 5.34 J/cm6.29 - 10.0 ft-lb/inAverage value: 4.04 J/cm Grade Count:5
Izod Impact, Notched (ISO) 7.00 - 15.0 kJ/m²3.33 - 7.14 ft-lb/in²Average value: 12.5 kJ/m² Grade Count:11
Charpy Impact Unnotched 3.00 - 4.00 J/cm²14.3 - 19.0 ft-lb/in²Average value: 3.44 J/cm² Grade Count:8
 3.00 - 4.00 J/cm²
@Temperature -30.0 - -30.0 °C
14.3 - 19.0 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 3.44 J/cm² Grade Count:8
Charpy Impact, Notched 0.399 - 1.40 J/cm²1.90 - 6.66 ft-lb/in²Average value: 1.01 J/cm² Grade Count:20
 0.800 - 1.30 J/cm²
@Temperature -30.0 - -30.0 °C
3.81 - 6.19 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 1.04 J/cm² Grade Count:8
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 100 - 1.00e+17 ohm-cm100 - 1.00e+17 ohm-cmAverage value: 1.13e+16 ohm-cm Grade Count:19
Surface Resistance 100 - 1.00e+16 ohm100 - 1.00e+16 ohmAverage value: 6.66e+15 ohm Grade Count:17
Dielectric Constant 2.90 - 3.302.90 - 3.30Average value: 3.08 Grade Count:5
Dielectric Strength 16.5 - 44.0 kV/mm420 - 1120 kV/inAverage value: 28.4 kV/mm Grade Count:7
Dissipation Factor 0.000400 - 0.001700.000400 - 0.00170Average value: 0.00102 Grade Count:5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 - 60.0 µm/m-°C7.80 - 33.3 µin/in-°FAverage value: 36.2 µm/m-°C Grade Count:21
CTE, linear, Transverse to Flow 52.2 - 75.6 µm/m-°C29.0 - 42.0 µin/in-°FAverage value: 64.2 µm/m-°C Grade Count:9
Thermal Conductivity 0.210 - 0.230 W/m-K1.46 - 1.60 BTU-in/hr-ft²-°FAverage value: 0.220 W/m-K Grade Count:7
Deflection Temperature at 0.46 MPa (66 psi) 130 - 160 °C266 - 320 °FAverage value: 140 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 105 - 148 °C221 - 298 °FAverage value: 129 °C Grade Count:35
Vicat Softening Point 138 - 165 °C280 - 329 °FAverage value: 145 °C Grade Count:11
UL RTI, Electrical 50.0 - 110 °C122 - 230 °FAverage value: 95.0 °C Grade Count:4
UL RTI, Mechanical with Impact 50.0 - 105 °C122 - 221 °FAverage value: 90.0 °C Grade Count:4
UL RTI, Mechanical without Impact 50.0 - 110 °C122 - 230 °FAverage value: 95.0 °C Grade Count:4
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:24
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 255 - 316 °C491 - 601 °FAverage value: 285 °C Grade Count:5
Melt Temperature 230 - 316 °C446 - 601 °FAverage value: 279 °C Grade Count:21
Mold Temperature 50.0 - 107 °C122 - 225 °FAverage value: 81.1 °C Grade Count:21
Drying Temperature 90.0 - 121 °C194 - 250 °FAverage value: 103 °C Grade Count:21
Moisture Content 0.0200 %0.0200 %Average value: 0.0200 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Polycarbonate, 30% Glass Filled
Overview of materials for Polypropylene Copolymer

O4891a / 89095

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.