MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wellman Wellamid® GFT33N051-N2 33% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/Nylon 6 Blend, Glass Fiber Filled

Material Notes: Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equipment.

Data provided by the manufacturer, Wellman Inc.

Key Words: Polyamide 66/6; Polyamide 6/66; Nylon 6/66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183
Water Absorption 1.2 %1.2 %Approximate 24 hr.
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 155 MPa22500 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Flexural Yield Strength 225 MPa32600 psiISO 178
Flexural Modulus 8.20 GPa1190 ksiISO 178
Izod Impact, Notched 1.30 J/cm2.44 ft-lb/inISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FISO 75
Flammability, UL94 HB
@Thickness 0.790 mm
HB
@Thickness 0.0311 in
From Wellman QC Laboratory Testing; UL 94

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Clariant Renol PA113G33 Nylon 66, 33% Glass Fiber, Heat Stabilized, Lubricated
Chase Plastics CP Pryme® NN133TL (Dry) Nylon 66, 33% Glass Fiber Reinforced, Lubricated, Impact Modified
Chase Plastics CP Pryme® NN133GTL (DAM) Nylon 66, 33% Glass Fiber Reinforced, Toughened, Internally Lubricated
PTS Trimid® N66-G33L 33% Glass Fiber Reinforced Lubed Nylon 6/6
PTS Trimid® N66-G33HL 33% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6

PWEL30 / 72310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.