MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Compression Grade
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: Sumikon® PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance and machinability. Typical applications include commutators.

Information provided by Sumitomo Bakelite North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.85 g/cc1.85 g/ccASTM D792
Bulk Density 0.700 g/cc0.0253 lb/in³ASTM D1895
Bulk Factor 2.62.6ASTM D1895
Water Absorption 0.050 %0.050 %ASTM D570
Linear Mold Shrinkage 0.0015 cm/cm0.0015 in/inASTM D6289
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 83.0 MPa12000 psiASTM D638
Tensile Modulus 15.2 GPa2200 ksiASTM D638
Flexural Strength 117 MPa17000 psiASTM D790
Compressive Strength 220 MPa31900 psiASTM D695
Izod Impact, Notched 0.480 J/cm0.899 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmASTM D257
Dielectric Constant  4.6
@Frequency 1e+6 Hz
4.6
@Frequency 1e+6 Hz
ASTM D150
 5.0
@Frequency 1000 Hz
5.0
@Frequency 1000 Hz
ASTM D150
 5.2
@Frequency 60 Hz
5.2
@Frequency 60 Hz
ASTM D150
Dielectric Strength 10.6 kV/mm270 kV/inStep by Step; ASTM D149
 11.8 kV/mm300 kV/inShort Time; ASTM D149
Dissipation Factor  0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
ASTM D150
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
ASTM D150
 0.030
@Frequency 60 Hz
0.030
@Frequency 60 Hz
ASTM D150
Arc Resistance 170 sec170 sec
Comparative Tracking Index 175 V175 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 227 °C441 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Injection Grade
Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade
Sumitomo Bakelite Durez® 25378 Phenolic, Compression Grade
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Compression Grade

P90X81 / 21198

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.