MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® B3 2 RM-D black (3254) PA 6 Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: AKROMID B3 2 RM-D black (3254) is a nonreinforced, UV-stabilized polyamide 6 with limited moisture absorption. Applications are interior and exterior parts with improved impact strength in the automotive industry

Additive: UV Stabilizer

Features:

  • Good Impact Resistance
  • Low Moisture Absorption
Uses:
  • Automotive Applications
  • Automotive Exterior Parts
  • Automotive Interiors

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Moisture Absorption 1.65 %
@Temperature 70.0 °C
1.65 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inISO 294-4
Melt Flow 30 g/10 min
@Load 5.00 kg,
Temperature 275 °C
30 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1183
Spiral Flow 65.0 cm25.6 inCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psi50 [mm/min]; ISO 527-2
Elongation at Break >= 30 %>= 30 %50 [mm/min]; ISO 527-2
Tensile Modulus 2.50 GPa363 ksi1 [mm/min]; ISO 527-2
Flexural Modulus 2.30 GPa334 ksi2 [mm/min]; ISO 178
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FDIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FUnannealed; ISO 75/B
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FUnannealed; ISO 75/A
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Nozzle Temperature 240 - 280 °C464 - 536 °F
Zone 1 225 - 300 °C437 - 572 °F
Zone 2 225 - 300 °C437 - 572 °F
Zone 3 225 - 300 °C437 - 572 °F
Zone 4 225 - 300 °C437 - 572 °F
Melt Temperature 260 - 300 °C500 - 572 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 - 12.0 hour4.00 - 12.0 hour
Hold Pressure 75.0 MPa10900 psi
Back Pressure 5.00 - 10.0 MPa725 - 1450 psi
 
Descriptive Properties
Resistance to AcetaldehydeFail100% Conc.
Resistance to Boric acidPass10% Conc
Resistance to Brake fluid (DOT 4)Pass10% Conc
Resistance to Dichloro-Acetic acidPass96% Conc
Resistance to Fruit JuicesPass50°C, 100% Conc
Resistance to Hydrogen chloride, gasPass100% Conc
Resistance to Iso-octanolPass100% Conc
Resistance to Oleic acidPass20% Conc
Resistance to Potassium permanganate, aqueousPass1% Conc
Resistance to SpiritsPass100% Conc
Resistance to TolueneFail100% Conc
Resistant to Citric acidPass10% Conc
Resistant to Hydrogen peroxideFail
Resistant to Sulfuric acidFail96% Conc
Resistant to WaterPass<50°C, 100% Conc
Resistant to Zinc chloride, aqueousPass50% Conc

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 2 RM-D (3374) PA 6 Dry
Akro-Plastic Akromid® B3 2 RM-D (3374) PA 6 Conditioned
A. Schulman SCHULAMID® 6 MV5 Unreinforced Nylon 6
A. Schulman SCHULAMID® 6 MV14 Unreinforced Nylon 6
Azoty Tarnow™ Tarnamid® T-30 Polyamide 6 - Natural

PAKRO241 / 182828

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.