MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem GM5340PRK Extrusion High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Description: GM5340PRK is a High Density Polyethylene compound specially developed for the manufacturing of ducts, subducts and jacketing for wires and cables. This resin is produced with bimodal technology and shows mechanical properties and resistance to stress cracking. GM5340PRK contains carbon black pigment that protects it against ultraviolet radiation action and photodegradation. The type and amount of carbon black used assure high UV absorption coefficient. It is also specially additivated to prevent copper catalytic oxidation.

Application: Jacketing for wires and optic fiber metallic cables; insulation of copper wires and cables; self-propelled irrigation pipes; localized irrigation pipes; ducts for mining.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.959 g/cc0.0346 lb/in³ASTM D792
ESCR 100% Igepal® >= 1000 hour
@Temperature 50.0 °C
>= 1000 hour
@Temperature 122 °F
F50, molded 2 mm, 0.3 mm notched-plaques; ASTM D1693
Carbon Black Loading 3.0 %3.0 %ASTM D1603
Melt Flow 0.55 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.55 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161ASTM D2240
Tensile Strength at Break 28.0 MPa4060 psiASTM D638
Tensile Strength, Yield 23.0 MPa3340 psiASTM D638
Elongation at Break 840 %840 %ASTM D638
Elongation at Yield 9.9 %9.9 %ASTM D638
Flexural Modulus, 1% Secant 980 MPa142000 psiASTM D790
Izod Impact, Notched 0.850 J/cm1.59 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmASTM D257
Dielectric Constant 2.6
@Frequency 1000 Hz
2.6
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 28.0 kV/mm711 kV/inASTM D149
Dissipation Factor 0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C154 °FASTM D648
Vicat Softening Point 121 °C
@Load 1.02 kg
250 °F
@Load 2.25 lb
ASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem GP5550BK HDPE High Density Extrusion Polyethylene
Braskem GD5150K HDPE High Density Extrusion Polyethylene
Borealis Borstar® CB9600 HDPE for Extrusion Coating
Braskem GP5550 HDPE High Density Extrusion Polyethylene
E-Glass Fiber, Generic

PBRASK2077 / 199958

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.