MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Caplinq LINQTAPE™ PIT2S
Categories: Polymer; Adhesive; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures.

Applications:

  • Temporary bonding of thermocouples for oven profiling
  • Bonding of devices prior to solder reflow
  • Insulating circuit boards
  • Masking in high temperature powder applications
  • Gold Finger Masking
  • Coil insulation
  • High temperature harness wrapping

Product Features and Benefits:

  • High temperature resistant
  • Excellent masking tape
  • Removes easily after high temperature exposure with no residues

Information provided by Caplinq

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 40.0 microns1.57 milAdhesive Thickness
 51.0 microns2.01 milFilm (Backing) Thickness
 91.0 microns3.58 milTotal Thickness
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 5.93 MPa860 psi13.5 N/25mm
Elongation at Break 60 %60 %
Adhesive Bond Strength 0.3297 MPa47.82 psi
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 118.3 kV/mm>= 3005 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air <= 260 °C<= 500 °F
Flammability, UL94 V-0V-0
 
Descriptive Properties
Adhesion TypeSilicone
ColorAmber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Caplinq LINQTAPE™ PIT1A
Caplinq LINQTAPE™ PIT1S
Caplinq LINQTAPE™ PIT2A
CEN® Electronic Material BL Polyimide Film
CEN® Electronic Material BX Polyimide Film

PCAPL004 / 90277

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.