MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Carborundum CarboTherm™ CTH30 Boron Nitride Powder
Categories: Ceramic; Nitride; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielectric properties at elevated temperatures. Applications include: use in potting compounds, encapsulants, epoxies, silicone oils and resins, and thermoplastics; use as a processing aid; use as a nucleating and foaming agent. Carborundum's CarboTherm™ powders can be custom blended to yield specific properties. Particle size and distribution can be tailored to give optimum fill and flowability while still maintaining high purity and consistency. CTH30 particles are platelets. Data provided by the manufacturer, Carborundum Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 0.700 g/cc0.0253 lb/in³Tap density
Particle Size 6.0 - 12 µm6.0 - 12 µmMean particle size
 
Component Elements PropertiesMetricEnglishComments
B2O3 0.20 %0.20 %
BN 97.6 %97.6 %
O2 0.50 %0.50 %includes the oxygen in B2O3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Trilac® ABS-HF5500 High Flow ABS Resin
Parabeam Industrie Paraglass 10 3D Glass Fabric
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Haynes 214® alloy, 20% cold reduction
ERG Aerospace Duocel® Aluminum Metal Foam

CBN005 / 652

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.