MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Cookson Group Plaskon® 2929BNSC Epoxy Molding Compound  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: Test specimens were transfer molded and post cured 4 hours at 175°C.

An epoxy molding compound for the encapsulation of semiconductor devices and fiber optics. Excellent moldability (good release, minimal flash and bleed, and good hot hardness); Superior cosmetics and markability; Outstanding reliability

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.92 g/cc0.0694 lb/in³
Spiral Flow 66.0 - 90.0 cm26.0 - 35.4 in177°C/1000 psi
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Flexural Strength 124 MPa18000 psi
Flexural Modulus 14.0 GPa2030 ksi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.2
@Frequency 1000 Hz
4.2
@Frequency 1000 Hz
Dielectric Strength 17.0 kV/mm432 kV/in
Dissipation Factor 0.0040
@Frequency 1000 Hz
0.0040
@Frequency 1000 Hz
Arc Resistance 180 sec180 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 27.0 µm/m-°C
@Temperature 20.0 °C
15.0 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.900 W/m-K6.25 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 145 °C293 °F
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 171 - 193 °C340 - 379 °FMolding temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Molding Compound
Cosmic Plastics CP7311 Epoxy Molding Compound
Cosmic Plastics E486 lass Filled Epoxy Molding Compound, Electrical Grade
Sumitomo Bakelite E 264H Epoxy Molding Compound
Cosmic Plastics FARBOSET® 2460 All Colors Mineral Filled Epoxy Molding Compound

PCOOK305 / 21401

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.