MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Techmer ES HiFill FR® PET GF15 IM FR X 15% Glass Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 20% Glass Reinforced

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass Fiber, 15% Filler by Weight

Additive: Impact Modifier and Mold Release

Features: Flame Retardant, Good Mold Release and Impact Modified

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.54 g/cc0.0556 lb/in³ASTM D792
Water Absorption 0.080 %
@Time 86400 sec
0.080 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm
@Thickness 3.17 mm
0.0060 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 34.5 MPa5000 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Flexural Yield Strength 6.89 MPa1000 psiASTM D790
Flexural Modulus 2.07 GPa300 ksiASTM D790
Izod Impact, Notched 0.801 J/cm
@Thickness 3.17 mm
1.50 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Strength 16.1 kV/mm410 kV/inMethod A (Short-Time); ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 12.6 µm/m-°C7.00 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 241 °C465 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 213 °C415 °FUnannealed; ASTM D648
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lavergne VYPET VNT 615 FR PET 15% Glass Reinforced, Flame Retardant
Eurotec® Tecopet® PT74 GR20 BK002 DA PET, 20% glass fiber reinforced, high heat stabilized, black
Eurotec® Tecopet® PT70 GR20 NL100 PR PET, 20% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Eurotec® Tecopet® PT70 GR15 NL100 PS20 PET, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade
Covestro Petlon® DP3-1039 Semi-Crystalline PET, 35% Glass Fiber

PTPC0742 / 136680

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.