MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Holmium, Ho
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 164.9303164.9303164.93032 - 1995
Atomic Number 6767
X-ray Absorption Edge 0.2229 Å0.2229 ÅK
 1.31942 Å1.31942 ÅLI
 1.38999 Å1.38999 ÅLII
 1.53529 Å1.53529 ÅLIII
Electronegativity 1.231.23Pauling
Ionic Radius 0.894 Å0.894 ÅCrystal Ionic Radius for Valence +3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 4646
Tensile Strength, Ultimate 259 MPa37600 psi
Tensile Strength, Yield 221 MPa32100 psi
Tensile Modulus 64.8 GPa9400 ksi
Bulk Modulus 40.2 GPa5830 ksi
Poissons Ratio 0.2310.231
Shear Modulus 26.3 GPa3810 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000814 ohm-cm0.0000814 ohm-cm
Magnetic Susceptibility 0.0004260.000426cgs/g
Curie Temperature -253 °C-423 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 104 J/g44.7 BTU/lb
CTE, linear 11.2 µm/m-°C
@Temperature 20.0 °C
6.22 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.163 J/g-°C0.0390 BTU/lb-°F
Thermal Conductivity 16.2 W/m-K112 BTU-in/hr-ft²-°FPolycrystalline Sample
Melting Point 1470 °C2680 °F
Boiling Point 2700 °C4890 °F
 
Component Elements PropertiesMetricEnglishComments
Holmium, Ho 100 %100 %
 
Descriptive Properties
CAS Number7440-60-0

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beryllium, Be
Americium, Am
Chromium, Cr; Recrystallized
Silver, Ag
Copper, Cu; Cold-Worked

AMEHo00 / 47

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.