MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Liquid
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive, Flexible

Material Notes: Epovex® Adhesive is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, Epovex is ideal for many metals, woods, masonry products and some plastics and rubbers. Epovex was also designed to bond Zyvex Technologies’ Arovex® composites. Additional fillers or glass micro-beads may be added to control sag qualities or to control bond-line thickness to a specific thickness or specification.

Features:

  • Excellent flexibility
  • Very high T-peel strengths
  • Very high tensile shear strengths
.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Shear Strength  15.9 MPa
@Temperature 60.0 °C
2300 psi
@Temperature 140 °F
Cure cycle: 7 days @ RT, with Aced Etched 6061-T6 Aluminum
 19.9 MPa
@Temperature 23.9 °C
2880 psi
@Temperature 75.0 °F
Cure cycle: 7 days @ RT (+7 days ethyl alcohol soak), with Aced Etched 6061-T6 Aluminum
 20.0 MPa
@Temperature 23.9 °C
2900 psi
@Temperature 75.0 °F
Cure cycle: 7 days @ RT (+7 days gasoline soak) , with Aced Etched 6061-T6 Aluminum
 20.3 MPa
@Temperature 23.9 °C
2940 psi
@Temperature 75.0 °F
6061-T6 Aluminum (abraded), with Arovex Carbon Fiber Epoxy Laminate
 22.1 MPa
@Temperature 23.9 °C
3200 psi
@Temperature 75.0 °F
Cure cycle: 3 days @ RT, with Aced Etched 6061-T6 Aluminum
 23.7 MPa
@Temperature 23.9 °C
3440 psi
@Temperature 75.0 °F
Arovex (abraded), with Arovex Carbon Fiber Epoxy Laminate
 24.0 MPa
@Temperature 23.9 °C
3480 psi
@Temperature 75.0 °F
Cure cycle: 7 days @ RT (+7 days water soak), with Aced Etched 6061-T6 Aluminum
 24.1 MPa
@Temperature 23.9 °C
3500 psi
@Temperature 75.0 °F
Cure cycle: 5 days @ RT, with Aced Etched 6061-T6 Aluminum
 24.4 MPa
@Temperature 23.9 °C
3540 psi
@Temperature 75.0 °F
Cure cycle: 7 days @ RT, with Aced Etched 6061-T6 Aluminum
 25.4 MPa
@Temperature 23.9 °C
3690 psi
@Temperature 75.0 °F
(+7 days water soak), with Arovex Carbon Fiber Epoxy Laminate
 27.6 MPa
@Temperature 23.9 °C
4000 psi
@Temperature 75.0 °F
Cure cycle: 12 hrs @ RT + 1 hr @ 176°F, with Aced Etched 6061-T6 Aluminum
 30.3 MPa
@Temperature -40.0 °C
4400 psi
@Temperature -40.0 °F
Cure cycle: 7 days @ RT, with Aced Etched 6061-T6 Aluminum
 31.1 MPa
@Temperature 23.9 °C
4510 psi
@Temperature 75.0 °F
Cure cycle: 2 hrs @ 176°F, with Aced Etched 6061-T6 Aluminum
Peel Strength 7.01 kN/m40.0 pliCure cycle: 1 day @ RT, with Acid Etched 6061-T6 Aluminum
 7.01 kN/m40.0 pliCure cycle: 12 hrs @ RT + 1 hr @ 176°F, with Acid Etched 6061-T6 Aluminum
 7.01 kN/m40.0 pliCure cycle: 3 days @ RT, with Acid Etched 6061-T6 Aluminum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum, Al
Nanocyl EPOCYL™ NC R128-04 Master Batch Liquid Bisphenol-A Resin for Solvent Based Formulation Purposes: Dilution Factor 6
Overview of materials for Epoxy/Carbon Fiber Composite
Nanocyl EPOCYL™ NC R1MY-02 Master Batch Liquid tetrafunctional epoxy Resin for Hot-Melt Formulation Purposes: Dilution Factor 6
Nanocyl EPOCYL™ NC R128-02 Master Batch Liquid Bisphenol-A Resin for Hot-Melt Formulation Purposes: Dilution Factor 6

PZYVEX92A / 159344

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.