MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Arkema Kynar Superflex® 2500-25 PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes:

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 - 1.82 g/cc1.80 - 1.82 g/ccASTM D792
Water Absorption <= 0.070 %<= 0.070 %ASTM D570
Viscosity 900000 - 1.60e+6 cP
@Shear Rate 100 1/s,
Temperature 230 °C
900000 - 1.60e+6 cP
@Shear Rate 100 1/s,
Temperature 446 °F
Melt; ASTM D3835
Melt Flow 1.0 - 15 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.0 - 15 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50 - 5750 - 57ASTM D2240
Tensile Strength at Break 13.8 - 31.0 MPa2000 - 4500 psiASTM D638
Tensile Strength, Yield 11.7 - 19.3 MPa1700 - 2800 psiASTM D638
Elongation at Break 500 - 800 %500 - 800 %ASTM D638
Elongation at Yield 17 - 25 %17 - 25 %ASTM D638
Tensile Modulus 0.241 - 0.379 GPa35.0 - 55.0 ksiASTM D638
Flexural Strength 10.3 - 17.2 MPa
@Strain 5.0 %
1490 - 2490 psi
@Strain 5.0 %
ASTM D790
Flexural Modulus 0.193 - 0.276 GPa28.0 - 40.0 ksiASTM D790
Compressive Strength 13.8 - 20.7 MPa2000 - 3000 psiASTM D695
Izod Impact, Notched NBNBASTM D256
Izod Impact, Unnotched NBNBASTM D256
Coefficient of Friction, Dynamic 0.540.54vs. steel; ASTM D1894
Coefficient of Friction, Static 0.490.49vs. steel; ASTM D1894
Taber Abrasion, mg/1000 Cycles 28 - 3328 - 33CS 17 1000g:pad; ASTM-G195-13A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm65% R.H; ASTM D257
Surface Resistivity per Square 8.50e+11 - 9.20e+11 ohm8.50e+11 - 9.20e+11 ohmASTM D257
Dielectric Constant 4.5 - 13.5
@Frequency 1000 Hz
4.5 - 13.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 0.800 - 1.10 kV/mm20.3 - 27.9 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 153 - 194 µm/m-°C85.0 - 108 µin/in-°FASTM D696
Specific Heat Capacity 0.745 - 0.958 J/g-°C0.178 - 0.229 BTU/lb-°FDSC
Thermal Conductivity 0.144 - 0.180 W/m-K0.999 - 1.25 BTU-in/hr-ft²-°FASTM D433
Melting Point 117 - 125 °C243 - 257 °FASTM D3418
Glass Transition Temp, Tg -41.7 - -40.0 °C-43.1 - -40.0 °FASTM D7028
Oxygen Index >= 75 %>= 75 %
 
Descriptive Properties
Form as DeliveredPellets
Moisture SensitiveNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARKF753a / 291168

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.