Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.54 g/cc | 1.54 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength | 1980 MPa | 287200 psi |
| 33.8 MPa @Temperature 132 °C | 4900 psi @Temperature 270 °F |
| 36.5 MPa @Temperature 71.0 °C | 5300 psi @Temperature 160 °F |
| 40.0 MPa @Temperature 24.0 °C | 5800 psi @Temperature 75.2 °F |
| 42.1 MPa @Temperature -54.0 °C | 6100 psi @Temperature -65.2 °F |
Tensile Modulus | 6.20 GPa @Temperature 132 °C | 899 ksi @Temperature 270 °F |
| 6.90 GPa @Temperature 71.0 °C | 1000 ksi @Temperature 160 °F |
| 8.30 GPa @Temperature 24.0 °C | 1200 ksi @Temperature 75.2 °F |
| 9.70 GPa @Temperature -54.0 °C | 1410 ksi @Temperature -65.2 °F |
| 121 GPa @Temperature -54.0 °C | 17500 ksi @Temperature -65.2 °F |
| 128 GPa @Temperature 24.0 °C | 18600 ksi @Temperature 75.2 °F |
| 129 GPa @Temperature 71.0 °C | 18700 ksi @Temperature 160 °F |
| 133 GPa @Temperature 132 °C | 19300 ksi @Temperature 270 °F |
Compressive Strength | 1172 MPa @Temperature 71.0 °C | 170000 psi @Temperature 160 °F |
| 1207 MPa @Temperature 24.0 °C | 175100 psi @Temperature 75.2 °F |
| 1241 MPa @Temperature 24.0 °C | 180000 psi @Temperature 75.2 °F |
| 1275 MPa @Temperature -54.0 °C | 184900 psi @Temperature -65.2 °F |
Compressive Modulus | 121 GPa @Temperature 132 °C | 17500 ksi @Temperature 270 °F |
| 123 GPa @Temperature 71.0 °C | 17800 ksi @Temperature 160 °F |
| 124 GPa @Temperature -54.0 °C | 18000 ksi @Temperature -65.2 °F |
| 124 GPa @Temperature 24.0 °C | 18000 ksi @Temperature 75.2 °F |
Shear Strength | 43.4 MPa @Temperature 132 °C | 6300 psi @Temperature 270 °F |
| 60.7 MPa @Temperature 132 °C | 8800 psi @Temperature 270 °F |
| 62.1 MPa @Temperature 71.0 °C | 9000 psi @Temperature 160 °F |
| 75.2 MPa @Temperature 24.0 °C | 10900 psi @Temperature 75.2 °F |
| 79.3 MPa @Temperature 71.0 °C | 11500 psi @Temperature 160 °F |
| 117 MPa @Temperature 24.0 °C | 17000 psi @Temperature 75.2 °F |
| 120 MPa @Temperature -54.0 °C | 17400 psi @Temperature -65.2 °F |
|
Thermal Properties | Metric | English | Comments |
---|
Maximum Service Temperature, Air | 149 °C | 300 °F |
|
Processing Properties | Metric | English | Comments |
---|
Processing Temperature | 177 °C @Time 7200 sec | 350 °F @Time 2.00 hour |
Shelf Life | 6.00 Month @Temperature -17.8 °C | 6.00 Month @Temperature 0.000 °F |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.