MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® B3 S1 natural (3715) PA 6 Conditioned, Cold-Impact Resistant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Description: AKROMID B3 S1 natural (3715) is a nonreinforced, cold impact strength polyamide 6 with light inherent color. Applications are mountings and dowels in the furniture and construction industry.

Features:

  • Low Temperature Impact Resistance
Uses:
  • Construction Applications
  • Furniture

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Moisture Absorption 2.0 %
@Temperature 70.0 °C
2.0 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.015 cm/cm0.015 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psi50 [mm/min]; ISO 527-2
Elongation at Break >= 100 %>= 100 %50 [mm/min]; ISO 527-2
Elongation at Yield 30 %30 %50 [mm/min]; ISO 527-2
Tensile Modulus 0.550 GPa79.8 ksi1 [mm/min]; ISO 527-2
Flexural Modulus 0.650 GPa94.3 ksi2 [mm/min]; ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 11.0 J/cm²
@Temperature 23.0 °C
52.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °FDIN EN 11357-1
 
Descriptive Properties
Resistant to Carbon tetrachloridePass100% Conc. at 23°C
Resistant to Citric acidPass10% Conc. at 23°C
Resistant to Ethyl acetatePass100% Conc. at 23°C
Resistant to Hydrochloric acidFail36% Conc. at 23°C
Resistant to Hydrogen peroxideFail23°C
Resistant to SeawaterPass100% Conc. at 23°C
Resistant to Silicone fluidPass23°C
Resistant to Sodium hypochlorite, aqueousFail5% Conc. at 23°C
Resistant to Sulfuric acidFail10% Conc. at 23°C
Resistant to Super-grade petrol (DIN 51600)Pass100% Conc. at 23°C
Resistant to ToluolPass100% Conc. at 23°C
Resistant to WaterPass100% Conc. up to 50°C
Resistant to XylolPass100% Conc. at 23°C
Resistant to Zinc chloride, aqueousFail50% Conc. at 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Capron® 8333G HI Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
BASF Capron® HPN 9315G HS BK-102 Impact Modified, 15% Glass-Filled Nylon 6 (Conditioned)
BASF Capron® 8351 Impact Modified Nylon 6 (Conditioned)
Akro-Plastic Akromid® B3 S1 black (3726) PA 6 Dry, Cold Impact Resistant
Akro-Plastic Akromid® B3 S1 black (3726) PA 6 Conditioned, Cold Impact Resistant

PAKRO349 / 182936

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.