MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Chemical Advanced Materials Nylatron™ FST PA66 Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Nylon shapes that are fire, smoke, and toxicity retardant, enabling them to withstand temperatures up to 347° F / 175° C. The first engineering plastic to achieve JAR / FAR 25.853 compliance, this polyimide grade was developed specifically for use in aircraft interior environments.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 88.088.0ASTM D785
Tensile Strength 90.0 MPa13100 psiISO 527-1/-2 (7)
Elongation at Yield 7.00 %7.00 %ISO 527-1/-2 (7)
Compressive Yield Strength  30.0 MPa
@Strain 1.00 %
4350 psi
@Strain 1.00 %
ISO 604 (10)
 60.0 MPa
@Strain 2.00 %
8700 psi
@Strain 2.00 %
ISO 604 (10)
 99.0 MPa
@Strain 5.00 %
14400 psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 0.490 J/cm²2.33 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 27.0 kV/mm686 kV/inIEC 60243-1 (15)
 
Thermal PropertiesMetricEnglishComments
CTE, linear  80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
 95.0 µm/m-°C
@Temperature 23.0 - 100 °C
52.8 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.280 W/m-K1.94 BTU-in/hr-ft²-°F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
Acids, Weak LimitedLimited
Alcohols LimitedLimited
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak LimitedLimited
Chlorinated Solvents LimitedLimited
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SM910 / 291067

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.