MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ASTM A148 Grade 150-135 Cast Steel
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: High Strength Castings for Structural Purposes

Key Words: 1035-930, D51350, SAE 8630
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 350350
Tensile Strength, Ultimate 1180 MPa171000 psi
Tensile Strength, Yield 1040 MPa151000 psi
Elongation at Break 8.0 %8.0 %
Reduction of Area 20 %20 %
Modulus of Elasticity 190 GPa27600 ksi
Poissons Ratio 0.290.29
Fatigue Strength 620 MPa89900 psi
Shear Modulus 73.0 GPa10600 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0000203 ohm-cm0.0000203 ohm-cmequal weight 8.5 % IACS
 0.0000233 ohm-cm0.0000233 ohm-cmequal volume 7.4 % IACS
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 250 J/g108 BTU/lb
CTE, linear 13.0 µm/m-°C7.22 µin/in-°F
Specific Heat Capacity 0.470 J/g-°C0.112 BTU/lb-°F
Thermal Conductivity 39.0 W/m-K271 BTU-in/hr-ft²-°F
Melting Point 1420 °C2590 °Fsolidus
 1460 °C2660 °Fliquidus
Maximum Service Temperature, Air 420 °C788 °Fmax mechanical
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.25 - 0.35 %0.25 - 0.35 %
Chromium, Cr 0.40 - 0.80 %0.40 - 0.80 %
Iron, Fe 96.1 - 98.2 %96.1 - 98.2 %
Manganese, Mn 0.60 - 1.0 %0.60 - 1.0 %
Molybdenum, Mo 0.15 - 0.30 %0.15 - 0.30 %
Nickel, Ni 0.40 - 0.80 %0.40 - 0.80 %
Phosphorus, P <= 0.050 %<= 0.050 %
Silicon, Si <= 0.60 %<= 0.60 %
Sulfur, S <= 0.060 %<= 0.060 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MASTMA148E / 313989

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.