MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66, 20% Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Carbon Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.14 - 1.50 g/cc0.0412 - 0.0542 lb/in³Average value: 1.24 g/cc Grade Count:51
Filler Content 15.0 - 20.0 %15.0 - 20.0 %Average value: 18.3 % Grade Count:12
Water Absorption 0.0100 - 6.00 %0.0100 - 6.00 %Average value: 1.06 % Grade Count:20
Moisture Absorption at Equilibrium 0.400 - 2.50 %0.400 - 2.50 %Average value: 1.98 % Grade Count:13
Water Absorption at Saturation 6.00 - 8.00 %6.00 - 8.00 %Average value: 6.59 % Grade Count:7
Additive Loading 15.0 - 20.0 %15.0 - 20.0 %Average value: 17.5 % Grade Count:4
Maximum Moisture Content  0.200 - 0.200
@Temperature 120 - 120 °C
0.200 - 0.200
@Temperature 248 - 248 °F
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
0.200 - 0.200
@Time 0.0830 - 0.0830 hour
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.000500 - 0.0180 cm/cm0.000500 - 0.0180 in/inAverage value: 0.00349 cm/cm Grade Count:40
 0.00200 - 0.00200 cm/cm
@Temperature 80.0 - 80.0 °C
0.00200 - 0.00200 in/in
@Temperature 176 - 176 °F
Average value: 0.00200 cm/cm Grade Count:2
Linear Mold Shrinkage, Transverse 0.00190 - 0.0110 cm/cm0.00190 - 0.0110 in/inAverage value: 0.00626 cm/cm Grade Count:13
 0.00600 - 0.00600 cm/cm
@Temperature 80.0 - 80.0 °C
0.00600 - 0.00600 in/in
@Temperature 176 - 176 °F
Average value: 0.00600 cm/cm Grade Count:2
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114 - 125114 - 125Average value: 119 Grade Count:11
Ball Indentation Hardness 160 - 270 MPa23200 - 39200 psiAverage value: 218 MPa Grade Count:4
Tensile Strength, Ultimate 104 - 255 MPa15100 - 37000 psiAverage value: 183 MPa Grade Count:45
 90.0 - 140 MPa
@Temperature 60.0 - 150 °C
13100 - 20300 psi
@Temperature 140 - 302 °F
Average value: 113 MPa Grade Count:1
Tensile Strength, Yield 104 - 230 MPa15100 - 33400 psiAverage value: 176 MPa Grade Count:8
Elongation at Break 1.00 - 13.0 %1.00 - 13.0 %Average value: 3.18 % Grade Count:52
 2.70 - 3.70 %
@Temperature 60.0 - 150 °C
2.70 - 3.70 %
@Temperature 140 - 302 °F
Average value: 3.35 % Grade Count:1
Modulus of Elasticity 4.30 - 19.0 GPa624 - 2760 ksiAverage value: 13.4 GPa Grade Count:43
 5.40 - 14.0 GPa
@Temperature 60.0 - 150 °C
783 - 2030 ksi
@Temperature 140 - 302 °F
Average value: 9.23 GPa Grade Count:1
Flexural Yield Strength 135 - 340 MPa19600 - 49300 psiAverage value: 268 MPa Grade Count:37
Flexural Modulus 6.55 - 16.5 GPa950 - 2390 ksiAverage value: 12.4 GPa Grade Count:36
Compressive Yield Strength 16.0 - 172 MPa2320 - 25000 psiAverage value: 88.1 MPa Grade Count:3
Izod Impact, Notched 0.534 - 1.92 J/cm1.00 - 3.60 ft-lb/inAverage value: 0.820 J/cm Grade Count:22
Izod Impact, Unnotched 5.34 - 9.08 J/cm10.0 - 17.0 ft-lb/inAverage value: 6.65 J/cm Grade Count:13
Izod Impact, Notched (ISO) 4.41 - 20.0 kJ/m²2.10 - 9.52 ft-lb/in²Average value: 9.20 kJ/m² Grade Count:10
 6.00 - 6.00 kJ/m²
@Temperature -30.0 - -30.0 °C
2.86 - 2.86 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 6.00 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 45.0 - 50.0 kJ/m²21.4 - 23.8 ft-lb/in²Average value: 48.3 kJ/m² Grade Count:3
 41.0 - 41.0 kJ/m²
@Temperature -30.0 - -30.0 °C
19.5 - 19.5 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 41.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.60 - 11.6 J/cm²12.4 - 55.2 ft-lb/in²Average value: 5.46 J/cm² Grade Count:19
 2.50 - 5.40 J/cm²
@Temperature -40.0 - -20.0 °C
11.9 - 25.7 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 3.97 J/cm² Grade Count:8
Charpy Impact, Notched 0.500 - 1.60 J/cm²2.38 - 7.61 ft-lb/in²Average value: 0.793 J/cm² Grade Count:18
 0.400 - 0.800 J/cm²
@Temperature -40.0 - -20.0 °C
1.90 - 3.81 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.569 J/cm² Grade Count:6
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0500 - 1.00e+12 ohm-cm0.0500 - 1.00e+12 ohm-cmAverage value: 2.94e+10 ohm-cm Grade Count:33
Surface Resistance 20.0 - 1.00e+10 ohm20.0 - 1.00e+10 ohmAverage value: 3.01e+8 ohm Grade Count:21
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.1 - 100 µm/m-°C6.70 - 55.6 µin/in-°FAverage value: 42.9 µm/m-°C Grade Count:15
Melting Point 221 - 266 °C430 - 511 °FAverage value: 258 °C Grade Count:21
Maximum Service Temperature, Air 100 - 240 °C212 - 464 °FAverage value: 151 °C Grade Count:8
Deflection Temperature at 0.46 MPa (66 psi) 200 - 260 °C392 - 500 °FAverage value: 249 °C Grade Count:16
Deflection Temperature at 1.8 MPa (264 psi) 200 - 259 °C392 - 498 °FAverage value: 247 °C Grade Count:39
Vicat Softening Point 230 - 260 °C446 - 500 °FAverage value: 251 °C Grade Count:8
Glass Transition Temp, Tg 5.00 - 72.0 °C41.0 - 162 °FAverage value: 40.4 °C Grade Count:3
Flammability, UL94 HB - V-0HB - V-0Grade Count:33
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 310 °C518 - 590 °FAverage value: 285 °C Grade Count:8
Melt Temperature 238 - 315 °C460 - 599 °FAverage value: 285 °C Grade Count:27
Mold Temperature 45.0 - 120 °C113 - 248 °FAverage value: 86.5 °C Grade Count:34
Drying Temperature 73.9 - 120 °C165 - 248 °FAverage value: 83.7 °C Grade Count:26
Moisture Content 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.170 % Grade Count:12
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:7
Injection Pressure 3.45 - 124 MPa500 - 18000 psiAverage value: 94.0 MPa Grade Count:14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
Overview of materials for Nylon 66, 10% Glass Fiber Filled
Overview of materials for Nylon 6, Carbon Fiber Filled

O2522 / 78021

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.